MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

American Elements Terbium Nanoparticles
Categories: Metal; Nonferrous Metal; Pure Element

Material Notes: General Description

Terbium (Tb) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Terbium Particles are typically 10 - 80 nanometers (nm) with specific surface area (SSA) in the 30 – 60 m 2 /g range. Nano Terbium Particles are also available in passivated and Ultra high purity and high purity and coated and dispersed forms. Research into applications for terbium nanocrystals has focused on use as a dopant in glass and optical fibers, in phosphors, nanophosphors and doped phosphorous nanoparticles i n nanosensors and nanodevices using caged atoms in nanoparticles doped with a few atoms of terbium as the emitter of green light and for their potential electrical, dielectric, magnetic, optical, imaging, catalytic, biomedical and bioscience properties and for use in coatings, plastics, nanowire, nanofiber and textiles and in alloy and catalyst applications.

Key Words: Formula: Tb; CAS Number: 7440-27-9
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.219 g/cc0.2969 lb/in³
Particle Size 0.010 - 0.080 µm0.010 - 0.080 µm
Specific Surface Area 30 - 60 m²/g30 - 60 m²/g
Molecular Weight 158.93 g/mol158.93 g/mol
 
Thermal PropertiesMetricEnglishComments
Melting Point 1356 °C2473 °F
Boiling Point 3230 °C5850 °F
 
Descriptive Properties
AppearanceBlack
StabilityExtremely reactive in air

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

EJAMER82 / 5565

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.