MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
A. Schulman Diamond Softflex® SF 7001 Thermoplastic Vulcanizate (TPV)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes:

A. Schulman has acquired Network Polymers & Diamond Polymers.

Key Words: Thermoplastic Elastomer Alloy
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.940 g/ccASTM D792
Linear Mold Shrinkage 0.014 - 0.016 cm/cm
@Thickness 3.17 mm
ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 70 - 80ASTM D2240
Tensile Strength at Break 4.80 MPachs 20 in/min; ASTM D412
Elongation at Break 650 %chs 20 in/min; ASTM D412
Compression Set 35 %
@Temperature 25.0 °C,
Time 79200 sec
ASTM D395

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
A. Schulman Diamond Softflex® SF 5591 Thermoplastic Vulcanizate (TPV)
Teknor Apex Sarlink® 3190 Thermoplastic Elastomer
ExxonMobil Geolast® 701-80W183 Thermoplastic Elastomer
ExxonMobil Santoprene® 171-73 Thermoplastic Elastomer
Teknor Apex Sarlink® 3135 Thermoplastic Elastomer

PDIAM499 / 126590

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.