MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Industeel UREA 316L Modified 316L Mod Low Si, High Mo Stainless Steel for Urea Plants
Categories: Metal; Ferrous Metal; Stainless Steel; T 300 Series Stainless Steel

Material Notes: Description: UREA 316L Modified grade has been specially developed for Urea plant applications. It is a 316L modified stainless steel with extra-low silicon content and substantial higher molybdenum contents. The low carbon content, combined with a well balanced chemistry (low silicon and nickel content close to 14%) makes the alloy fully austenitic, free of intermetallic phase precipitations. The ferrite level is kept under 0.5% in the solution annealing and water quenched conditions. The alloy is designed for improved corrosion resistance properties in Ureacarbonate environments.

Information provided by manufacturer.

Key Words: EN 10088 / EN 10028 X2 Cr Ni Mo 18-14-3 - 1.4435, AFNOR Z3 CND 18.14.03, DIN W.Nr 1.4435, ASTM 316L modified
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.90 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate >= 490 MPaMinimum Guaranteed
 530 MPaTypical after Solution Annealing
Tensile Strength, Yield >= 190 MPaMinimum Guaranteed
 250 MPa
@Strain 0.2 %
Typical after Solution Annealing
 280 MPa
@Strain 1 %
Typical after Solution Annealing
Elongation at Break 55 %Typical
Modulus of Elasticity 200 GPa
Poissons Ratio 0.333Calculated
Shear Modulus 75.0 GPa
@Temperature 20.0 °C
Charpy Impact >= 120 J
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000740 ohm-cm
@Temperature 20.0 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 16.0 µm/m-°C
@Temperature 20.0 - 100 °C
 16.5 µm/m-°C
@Temperature 20.0 - 300 °C
 17.5 µm/m-°C
@Temperature 20.0 - 500 °C
Specific Heat Capacity 0.500 J/g-°C
@Temperature 20.0 °C
Thermal Conductivity 15.0 W/m-K
@Temperature 20.0 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.030 %
Chromium, Cr 18 %
Iron, Fe 63.37 - 64.9 %As remainder
Manganese, Mn 1.0 - 2.0 %
Molybdenum, Mo 2.6 %
Nickel, Ni 13.5 %
Silicon, Si <= 0.50 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
310 Stainless Steel, annealed sheet
Industeel VIRGO 39 16% Cr, 5% Ni, Martensitic Stainless Steel
Outokumpu 4435 Cr-Ni-Mo Austenitic Stainless Steel
Industeel SIRIUS 310 25% Cr - 0.6% Si Heat Resistant Stainless Steel
Bisalloy Steels BisPlate 80PV Thickness >80-100 mm

NINDUST36 / 17574

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.