MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Industeel VIRGO 17.4PH 17Cr-4Ni-3Cu Precipitation Hardening Martensitic Stainless Steel (593°C - 4 hours + air cooled)
Categories: Metal; Ferrous Metal; Martensitic; Stainless Steel; Precipitation Hardening Stainless; T S10000 Series Stainless Steel

Material Notes: Description: Alloy VIRGO 17.4 PH is a precipitation hardening martensitic stainless steel with Cu and Nb/Cb additions. The grade combines high strength, hardness (up to 300°C / 572°F) and corrosion resistance. Mechanical properties can be optimized with heat treatment. Very high yield strength up to 1100-1300 MPa can be achieved. The grade should not be used at temperatures above 300°C (572°F) or at very low temperatures. It has adequate resistance to atmospheric corrosion or in diluted acids or salts where its corrosion resistance is equivalent to CLC 18.9 (304) or SOLEIL B4 (430). If there are potential risks of stress corrosion cracking, higher aging temperatures must be selected over 550°C (1022°F), preferably 590°C(1094°F). The main applications are :
  • mechanical components
  • aerospace
  • offshore industry
  • food industry

Information provided by manufacturer.

Key Words: EURONORM 1.4542 X5CrNiCuNb 16-4, AFNOR Z5 CNU 17-4PH, DIN 1.4542, ASTM A693 grade 630 (AMS 5604B), UNS S17400
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.80 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 293Typical
Hardness, Rockwell C 29Typical
Tensile Strength, Ultimate >= 965 MPaMinimum Guaranteed
 1034 MPaTypical
Tensile Strength, Yield >= 790 MPa
@Strain 0.2 %
 931 MPa
@Strain 0.2 %
Typical
Elongation at Break >= 10 %
 17 %Typical
Charpy Impact >= 20.0 JAt RT, Transverse
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.040 %
Chromium, Cr 16.5 %
Copper, Cu 3.3 %
Iron, Fe 74.66 %As remainder
Manganese, Mn 0.70 %
Nickel, Ni 4.5 %
Niobium, Nb (Columbium, Cb) 0.30 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Industeel VIRGO 17.4PH 17Cr-4Ni-3Cu Precipitation Hardening Martensitic Stainless Steel (496°C - 4 hours + air cooled)
Industeel VIRGO 17.4PH 17Cr-4Ni-3Cu Precipitation Hardening Martensitic Stainless Steel (480°C (900°F) - 1 hour + air cooled)
Aluminum 355.0-T61, Cast
FloMet 17-4PH Stainless Steel, Heat Treated (H-900)
Special Metals INCONEL® Alloy HX

NINDUST24 / 17562

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.