MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
CP-Polymer-Technik Wellamid® 6600 MF30 HWCP 30% Milled Glass Fiber Nylon 66, Heat Stabilized, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled

Material Notes: Information provided by CP-Polymer-Technik GmbH & Co. KG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.36 g/ccISO 1183
Moisture Absorption at Equilibrium 1.8 - 2.3 %23°C/50%RH; DIN 53495
Linear Mold Shrinkage 0.0050 cm/cm
@Thickness 4.00 mm
Linear Mold Shrinkage, Transverse 0.0070 cm/cm
@Thickness 4.00 mm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 130 MPa5 mm/min; ISO 527
Elongation at Break 3.0 %5 mm/min; ISO 527
Tensile Modulus 7.50 GPaISO 527
Flexural Modulus 6.20 GPaDIN 52457
Charpy Impact Unnotched 3.50 J/cm²
@Temperature 23.0 °C
ISO 179
Charpy Impact, Notched 0.800 J/cm²
@Temperature 23.0 °C
ISO 179
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmIEC 93
Surface Resistance 1.00e+12 ohmISO 3915
Dielectric Constant 4.0
@Frequency 1e+6 Hz
IEC 250
Dielectric Strength 35.0 kV/mmIEC 243-1
Dielectric Loss Index 0.015
@Frequency 1e+6 Hz
IEC 250
Comparative Tracking Index 550 VStufe; IEC 112
 
Thermal PropertiesOriginal ValueComments
CTE, linear 30.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
DIN 53752
Melting Point 255 °CKofler
Deflection Temperature at 0.46 MPa (66 psi) 250 °CISO 179
Deflection Temperature at 1.8 MPa (264 psi) 200 °CISO 179
Vicat Softening Point 230 °C50 N; ISO 306
Flammability, UL94 HB
@Thickness 1.60 mm
Stufe; IEC 707
 HB
@Thickness 3.20 mm
Stufe; IEC 707
 
Processing PropertiesOriginal ValueComments
Melt Temperature 265 - 295 °C
Mold Temperature 70.0 - 100 °C
 
Descriptive Properties
Back PressureLow
Holding PressureHigh
Injection SpeedHigh
Screw SpeedMedium

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
CP-Polymer-Technik Wellamid® 6000 MF 30 HWCP 30% Milled Glass Fiber Nylon 6, Heat Stabilized, Dry
CP-Polymer-Technik Wellamid® 6000 MF 30 HWCP 30% Milled Glass Fiber Nylon 6, Heat Stabilized, Conditioned
CP-Polymer-Technik Wellamid® 6600 MF30 HWCP 30% Milled Glass Fiber Nylon 66, Heat Stabilized, Conditioned
Techmer ES HiFill® PA6 GF30 L 30% Milled Glass
Techmer ES HiFill® PA6 GF40 L 40% Milled Glass

PWELL166 / 72623

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.