MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
Momentive Performance Materials SilCool™ LTR3291 Low Thermal Resistance Silicone Adhesive  (discontinued **)
Categories: Polymer; Adhesive; Thermoset; Silicone; Silicone, RTV, Adhesive/Sealant Grade

Material Notes: SilCoolTM LTR3291 silicone adhesive is a one-component, medium viscosity, thermally conductive material, that will remain in a liquid, uncured state at room temperature, curing to an elastomer when sufficient heat is applied.

SilCool LTR3291 silicone adhesive provides much higher thermal conductivity than conventional silicone adhesives; making it suitable for use in electrical and electronic applications where thermal management and high heat transfer is critical. Utilizing a specially developed filler technology, SilCool LTR3291 is capable of achieving a reduced bond line thickness and has very low thermal resistance values. It is non-corrosive to metals and has excellent adhesive properties to a wide variety of substrates, including ceramics, glass, and most metals, including aluminum, copper and nickel plate. In addition, it also offers excellent adhesion to a broad range of high performance thermoplastics, such as PPS and PBT.

Key Performance Properties:

  • Excellent thermal conductivity properties
  • Very low thermal resistance
  • Reduced bond line thickness capability (< 2 mils)
  • Heat accelerated cure, one component, to increase productivity
  • Primerless adhesion eliminates mechanical fastening
  • Outstanding long-term performance under high humidity

GE Silicones became a part of Momentive Performance Materials in 2006.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.82 g/cc
@Temperature 23.0 °C
Viscosity 60000 cP10.0/s, CSL2500 Rheometer
 385000 cP1.0/s, CSL2500 Rheometer
 1.35e+6 cP0.10/s, CSL2500 Rheometer
Brookfield Viscosity 260000 cP
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 92
Tensile Strength at Break 2.30 MPa
Elongation at Break 15 %
Adhesive Bond Strength 100 psiAluminum lap shear, 1" overlap at 0.125" thickness, 30 min. at 150°C
 300 psiDie shear, Si die to aluminum shear, 2 hrs. at 150°C
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.63e+16 ohm-cm
Dielectric Constant 5.7
@Frequency 1000 Hz
Dielectric Strength 16.6 kV/mm
Dissipation Factor 0.0020
@Frequency 1000 Hz
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 2.37 W/m-KBulk
 
Descriptive Properties
ColorGray
ConsistencySemi-flowable
Ionic content<5ppmNa+,K+,Cl+, uncured samples
Thermal Resistance24 mm2K/Wat 23°C

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ampco Metal AMPCO® 45 Nickel-Aluminum Bronze, Extruded and Drawn Rods, ≤ 25.4 mm.
Momentive Performance Materials TSE3280G Thermally Conductive, Heat Cured Silicone Adhesive
Dow 3-6651 THERMALLY CONDUCTIVE ELASTOMER, KIT
Dow FLUOROGEL® Q3-6679 DIELECTRIC GEL KIT
Kinetics MIM F15 (Kovar™) Low CTE Alloy

PGESIL064 / 41055

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.