MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Acrylic, Impact Modified, Molded
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Acrylic, Impact Modified, Molded

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Impact Modified, Molded". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.04 - 1.19 g/cc0.0376 - 0.0430 lb/in³Average value: 1.16 g/cc Grade Count:148
Water Absorption 0.100 - 3.00 %0.100 - 3.00 %Average value: 0.380 % Grade Count:83
Moisture Absorption at Equilibrium 0.300 - 0.400 %0.300 - 0.400 %Average value: 0.360 % Grade Count:7
Water Absorption at Saturation 0.300 %0.300 %Average value: 0.300 % Grade Count:6
Viscosity  975000 - 975000 cP
@Temperature 240 - 240 °C
975000 - 975000 cP
@Temperature 464 - 464 °F
Average value: 975000 cP Grade Count:1
 975000 - 975000 cP
@Shear Rate 100 - 100 1/s
975000 - 975000 cP
@Shear Rate 100 - 100 1/s
Average value: 975000 cP Grade Count:1
Linear Mold Shrinkage 0.00200 - 0.00900 cm/cm0.00200 - 0.00900 in/inAverage value: 0.00510 cm/cm Grade Count:126
Melt Flow 0.300 - 22.0 g/10 min0.300 - 22.0 g/10 minAverage value: 4.10 g/10 min Grade Count:146
Spiral Flow 22.0 - 46.0 cm8.66 - 18.1 inAverage value: 29.9 cm Grade Count:14
 130 - 330 cm
@Temperature 230 - 250 °C
51.2 - 130 in
@Temperature 446 - 482 °F
Average value: 228 cm Grade Count:8
 130 - 330 cm
@Thickness 2.00 - 2.00 mm
51.2 - 130 in
@Thickness 0.0787 - 0.0787 in
Average value: 228 cm Grade Count:8
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 20.0 - 95.020.0 - 95.0Average value: 59.7 Grade Count:72
Hardness, Rockwell R 61.0 - 11861.0 - 118Average value: 92.9 Grade Count:17
Tensile Strength, Ultimate 30.0 - 82.0 MPa4350 - 11900 psiAverage value: 50.1 MPa Grade Count:128
Tensile Strength, Yield 28.0 - 68.0 MPa4060 - 9860 psiAverage value: 44.4 MPa Grade Count:21
Elongation at Break 1.90 - 90.0 %1.90 - 90.0 %Average value: 30.7 % Grade Count:144
Elongation at Yield 1.90 - 40.0 %1.90 - 40.0 %Average value: 5.74 % Grade Count:39
Modulus of Elasticity 1.30 - 3.52 GPa189 - 510 ksiAverage value: 2.13 GPa Grade Count:115
Flexural Yield Strength 46.0 - 113 MPa6670 - 16400 psiAverage value: 72.5 MPa Grade Count:132
Flexural Modulus 1.30 - 3.38 GPa189 - 490 ksiAverage value: 2.12 GPa Grade Count:95
Izod Impact, Notched 0.196 - 2.45 J/cm0.367 - 4.59 ft-lb/inAverage value: 0.572 J/cm Grade Count:95
 0.240255 - 0.37373 J/cm
@Temperature 0.000 - 0.000 °C
0.450096 - 0.70015 ft-lb/in
@Temperature 32.0 - 32.0 °F
Average value: 0.330 J/cm Grade Count:6
 0.260 - 0.590 J/cm
@Temperature 0.000 - 0.000 °C
0.487 - 1.11 ft-lb/in
@Temperature 32.0 - 32.0 °F
Average value: 0.330 J/cm Grade Count:2
 0.260 - 0.590 J/cm
@Thickness 6.35 - 6.35 mm
0.487 - 1.11 ft-lb/in
@Thickness 0.250 - 0.250 in
Average value: 0.330 J/cm Grade Count:2
 0.210 - 0.64068 J/cm
@Diameter 6.35 - 6.35 mm
0.393 - 1.2003 ft-lb/in
@Diameter 0.250 - 0.250 in
Average value: 0.330 J/cm Grade Count:10
 0.210 - 0.64068 J/cm
@Temperature 0.000 - 0.000 °C
0.393 - 1.2003 ft-lb/in
@Temperature 32.0 - 32.0 °F
Average value: 0.330 J/cm Grade Count:10
Izod Impact, Unnotched 1.60 J/cm - NB3.00 ft-lb/in - NBAverage value: 3.92 J/cm Grade Count:7
 2.45166 - 2.54973 J/cm
@Temperature 0.125 - 0.250 °C
4.59297 - 4.77669 ft-lb/in
@Temperature 32.2 - 32.5 °F
Average value: 2.50 J/cm Grade Count:1
Izod Impact, Notched (ISO) 2.10 - 8.00 kJ/m²0.999 - 3.81 ft-lb/in²Average value: 4.43 kJ/m² Grade Count:19
Izod Impact, Unnotched (ISO) 1.50 - 9.20 kJ/m²0.714 - 4.38 ft-lb/in²Average value: 4.31 kJ/m² Grade Count:13
Charpy Impact Unnotched 2.10 - 15.0 J/cm²9.99 - 71.4 ft-lb/in²Average value: 5.81 J/cm² Grade Count:48
Charpy Impact, Notched 0.120 - 0.850 J/cm²0.571 - 4.05 ft-lb/in²Average value: 0.431 J/cm² Grade Count:47
Gardner Impact 1.58 - 11.0 J1.17 - 8.11 ft-lbAverage value: 4.74 J Grade Count:48
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+12 - 1.00e+17 ohm-cm1.00e+12 - 1.00e+17 ohm-cmAverage value: 4.60e+15 ohm-cm Grade Count:24
Surface Resistance 1.00e+14 - 1.00e+16 ohm1.00e+14 - 1.00e+16 ohmAverage value: 5.38e+15 ohm Grade Count:15
Dielectric Constant 2.50 - 3.902.50 - 3.90Average value: 3.40 Grade Count:24
Dielectric Strength 15.0 - 60.0 kV/mm381 - 1520 kV/inAverage value: 26.1 kV/mm Grade Count:24
Dissipation Factor 0.0100 - 0.05000.0100 - 0.0500Average value: 0.0408 Grade Count:24
Comparative Tracking Index 600 V600 VAverage value: 600 V Grade Count:7
 
Thermal PropertiesMetricEnglishComments
CTE, linear 38.0 - 123 µm/m-°C21.1 - 68.3 µin/in-°FAverage value: 89.3 µm/m-°C Grade Count:94
 72.0 - 93.6 µm/m-°C
@Temperature 0.000 - 156 °C
40.0 - 52.0 µin/in-°F
@Temperature 32.0 - 312 °F
Average value: 78.6 µm/m-°C Grade Count:6
Specific Heat Capacity 1.30 - 1.50 J/g-°C0.311 - 0.359 BTU/lb-°FAverage value: 1.48 J/g-°C Grade Count:9
 1.90 - 2.30 J/g-°C
@Temperature 100 - 175 °C
0.454 - 0.550 BTU/lb-°F
@Temperature 212 - 347 °F
Average value: 2.10 J/g-°C Grade Count:1
Thermal Conductivity 0.200 - 0.220 W/m-K1.39 - 1.53 BTU-in/hr-ft²-°FAverage value: 0.203 W/m-K Grade Count:12
Maximum Service Temperature, Air 50.0 - 99.0 °C122 - 210 °FAverage value: 81.9 °C Grade Count:27
Deflection Temperature at 0.46 MPa (66 psi) 78.0 - 187 °C172 - 369 °FAverage value: 94.8 °C Grade Count:16
Deflection Temperature at 1.8 MPa (264 psi) 73.0 - 190 °C163 - 374 °FAverage value: 85.7 °C Grade Count:124
Vicat Softening Point 78.0 - 115 °C172 - 239 °FAverage value: 101 °C Grade Count:142
Heat Distortion Temperature 80.0 - 97.0 °C176 - 207 °FAverage value: 90.3 °C Grade Count:8
Flammability, UL94 HBHBGrade Count:65
Oxygen Index 18.0 - 19.0 %18.0 - 19.0 %Average value: 18.2 % Grade Count:6
Glow Wire Test 650 - 675 °C1200 - 1250 °FAverage value: 651 °C Grade Count:20
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.49 - 1.571.49 - 1.57Average value: 1.50 Grade Count:72
Haze 0.400 - 97.0 %0.400 - 97.0 %Average value: 4.72 % Grade Count:100
Yellow Index -1.50 - 5.50 %-1.50 - 5.50 %Average value: 0.879 % Grade Count:19
Transmission, Visible 0.000 - 92.0 %0.000 - 92.0 %Average value: 86.7 % Grade Count:122
UV Transmittance 91.0 - 92.0 %91.0 - 92.0 %Average value: 91.8 % Grade Count:13
 
Processing PropertiesMetricEnglishComments
Processing Temperature 210 - 250 °C410 - 482 °FAverage value: 230 °C Grade Count:8
Melt Temperature 179 - 260 °C354 - 500 °FAverage value: 229 °C Grade Count:43
Mold Temperature 26.7 - 107 °C80.0 - 225 °FAverage value: 60.8 °C Grade Count:41
Drying Temperature 60.0 - 105 °C140 - 221 °FAverage value: 80.8 °C Grade Count:35
Injection Pressure 49.0 - 108 MPa7110 - 15700 psiAverage value: 79.4 MPa Grade Count:9
Annealing Temperature 60.0 - 70.0 °C140 - 158 °FAverage value: 65.0 °C Grade Count:8

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Acrylic, General Purpose, Molded
Overview of materials for Acrylic, Extruded
Overview of materials for Cellulose Acetate, Molded
Overview of materials for Acrylic, UV Stabilized, Molded
Overview of materials for Polycarbonate, Molded

O1302 / 77861

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.