MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Industrial Nanotech Nansulate™ GP Translucent Insulation Coating
Categories: Ceramic; Other Engineering Material; Ceramic/Metallic Coating

Material Notes: Liquid insulation and corrosion protection incorporating Hydro-NM-Oxide, a product of nanotechnology. This grade is for general purpose insulation.

NANSULATE™ liquid applied insulation is a premium industrial grade rust proofing protective insulation coating containing Hydro-NM-Oxide. NANSULATE™, when fully cured, contains a high level of Hydro-NM-Oxide along with acrylic resin and performance additives. Nansulate has proven resistance to both existing mold growth and new mold growth. Nansulate can also be used for Lead Abatement—as a lead encapsulation coating. 20 year warranty.

Uses: Pipes, Tanks, Trucks, Textile, Attics, Walls, Ships, Automotive, Containers, Residential, Commercial, Industrial

Corrosion protection and insulation are now combined into one, solving the costly problem of CUI (corrosion under insulation).
Excellent adhesion to a wide variety of substrates.
User-friendly with no special tools needed and easy to apply.
Effective three-coat system, which can be easily over-coated if desired.
Ability to see the substrate through the material allows for visual inspection of pipes, tank and equipment.
Mold resistance without use of potentially harmful anti-fungal agents
Encapsulate Lead with a smooth, water-based, environmentally friendly coating.

Information provided by Industrial Nanotech, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.02 g/cc0.0368 lb/in³as supplied
Solids Content 28 - 32 %28 - 32 %By Volume
 30 - 34 %30 - 34 %By Weight
Viscosity 3500 - 4000 cP3500 - 4000 cPas supplied
Thickness 76.2 - 127 microns3.00 - 5.00 milper coat; minimum three coats recommended
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.0180 W/m-K0.125 BTU-in/hr-ft²-°Fcured coating
Maximum Service Temperature, Air 125 °C257 °Fcured coating
 
Processing PropertiesMetricEnglishComments
Processing Temperature 4.00 - 100 °C39.2 - 212 °FApplication Temperature
Cure Time 60.0 - 120 min1.00 - 2.00 hourHand Dry
 1440 - 2880 min24.0 - 48.0 hourhard dry (return to service)
 43200 - 86400 min720 - 1440 hourfull cure
 
Descriptive Properties
ColorTranslucent
Coverage per gallon150 - 175 sq. ft. with three coats

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Industrial Nanotech Nansulate™ High Heat Translucent Insulation Coating
Industrial Nanotech Nansulate™ PT Translucent Insulation Coating
3M K37 Glass Bubbles
3M K25 Glass Bubbles
3M S38HS Glass Bubbles

CINDNAN02 / 1389

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.