MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Gabriel Fluorolube® GR-290 CTFE Fluoropolymer Grease
Categories: Fluid; Lubricant; Fluoropolymer Base

Material Notes: Fluorolube® greases are liquid lubricants that deliver long-lasting lubrication for metallic surfaces (except copper, aluminum and magnesium) in applications requiring stability and performance in strongly acidic and/or oxidizing environments. They are saturated, hydrogen-free, low-molecular weight polymers of chlorotrifluoroethylene (CTFE). Available in a range of viscosities for demanding conditions, Fluorolube® greases are compatible with chlorine, oxygen, hydrogen peroxide, red fuming nitric acid and other strong oxidizing agents, and are nonflammable.

Information provided by Gabriel Chemical.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Penetration 229 - 249
@Temperature 25.0 °C
0.1 mm; ASTM D-217-82
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 150 °Cdepends on time and environment
Minimum Service Temperature, Air -20.0 °C
Dropping Point 280 °CASTM D2265
 
Descriptive Properties
CAS Number9002-83-9

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Mitsubishi Chemical Advanced Materials Duratron™ D7000 PI Unfilled Polyimide
Daikin NEOFLON® M-300H PCTFE Granular Molding Powder
Dow MOLYKOTE® 1292 LONG LIFE BEARING GREASE
Gabriel Gabepro® GPM-888 Mercaptan Epoxy Curing Agent Formulation
Gabriel Gabepro® GPM-800 Mercaptan Epoxy Curing Agent

VGABR880 / 230692

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.