MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Go Yen Chemical CL-220 Lubricant Additives For Plastic
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Intro: CL-220 is a transparent processing additive with comprehensive applications. It can provide good lubrication to plastic products, including internal and external lubrication. It can enhance the injection and extrusion capability of products, increasing the production efficiency and the flow of resin. Our capacity reach 200 tons per month, and we supply to domestic and overseas PVC, ABS, PS, TPU producer and engineering plastics granulation companies.

Characteristics:

  • Good internal and external lubricant processing additive
  • Increase the product flow stability and productivity
  • Improve the process of granulation for a variety of plastic pellets and additives or Filler (filler).
  • Apply to shrink film or packing blown
  • Perfect transparency and increase the thermal stability of products
  • With internal and external lubrication, it can improve the long-term processability of Tin stabilizer.
  • Without adding additional lubrication and heat stabilizer.
  • Improve the plate out and surface smoothness and increase speed of productivity.
  • Increase the products smooth and good antideterioration of processing
Applications:
  • PVC lubricant
  • R-PVC lubricant
  • PVC wire/cable lubricant
  • PS.EPS.HIPS.GPPS Processing lubricants
  • Application of ABS granulation
  • Apply to various extrusion, injection and filmprocessing
  • Thermoplastic polyurethane elastomers (TPU)
  • PVC.PP.PE.EVA.POE…polyolefin products
  • Engineering plastics: Nylon, PET, PC, POM
  • Various thermoplastic products
  • Thermosetting products: Phenolic resin, epoxy, melamine, unsaturated resin ….etc.
  • Processing additives and lubricant additives for general plastic and engineering plastics
  • Coatings, resins, inks, processing additives

Information provided by Go Yen Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Chemical PropertiesMetricEnglishComments
Acid Value <= 0.10<= 0.10[mg KOH/g]
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.050 %<= 0.050 %
 
Descriptive Properties
AppearanceTransparent Clear
Color<30APHA
Purity99.5%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PGOYEN326 / 266634

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.