MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Greene Tweed CHEMRAZ® 661 Perfluoroelastomer
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Material Notes: Chemraz® 661 perfluoroelastomer is specifically developed by Greene Tweed to meet the unique demands of aggressive plasma systems. This product’s unique formulation provides enhanced plasma resistance and reduced contamination resulting in less downtime and lower cost of ownership. Chemraz 661 is recommended for both static and dynamic dry wafer processing applications such as etch and CVD. Chemraz 661 remains stable at service temperatures up to 240°C (464°F).

Applications:

  • Window seals
  • Bell jar seals
  • Valve seals
  • KF fitting seals
  • Isolator valve seals
  • Lid seals
  • Gas inlet seals
  • Slit valve seals

Information provided by Greene Tweed.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.11 g/ccASTM D297
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 80ASTM D2240
Tensile Strength at Break 2620 psiASTM D1414
Tensile Strength, Yield 400 psi@50% Elongation; ASTM D1414
 1200 psi@100% Elongation; ASTM D1414
Elongation at Break 140 %ASTM D1414
Compression Set 17 %
@Temperature 204 °C,
Time 252000 sec
At 25% deflection; ASTM D395
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 464 °F
Minimum Service Temperature, Air -4.00 °F
 
Descriptive Properties
ColorWhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Greene Tweed CHEMRAZ® 653 Perfluoroelastomer
Greene Tweed CHEMRAZ® 555 Perfluoroelastomer
Greene Tweed CHEMRAZ® E38 Perfluoroelastomer
Greene Tweed CHEMRAZ® 656 Perfluoroelastomer
Greene Tweed CHEMRAZ® 655 Perfluoroelastomer

PGREEN33 / 42327

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.