MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese Celanex® 3116 PBT, 7.5% Glass Reinforced
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled

Material Notes: Celanex 3116 is a non-exuding flame retarded (UL and CSA approved V-0 at 1/32 inch and 5V at 1/8 inch), 7.5% fiberglass reinforced polybutylene terephthalate which has an excellent balance of mechanical properties and processability. It is well suited for
To avoid hydrolytic degradation during processing, CELANEX resins have to be dried to a moisture level equal to or less than 0.02%. Drying should be done in a dehumidifying hopper dryer capable of dewpoints <-40°F (-40°C) at 250°F (121°C) for 4 hours.
For subsequent storage of the material in the dryer until processed (<= 60 h) it is necessary to lower the temperature to 100° C.

Information provided by Celanese Corporation.

Key Words: 7.5% glass-fiber, V-0, non-exuding
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.50 g/ccASTM D792
Density 1.50 g/ccISO 1183
Moisture Absorption at Equilibrium 0.20 %23°C/50%RH; ISO 62
Linear Mold Shrinkage, Flow 0.010 - 0.014 cm/cmISO 294-4
 0.010 - 0.014 in/inASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 83ISO 2039-2
Tensile Strength at Break 75.0 MPa5mm/min; ISO 527-2/1A
 11000 psi
@Temperature 22.8 °C
ASTM D638
Tensile Stress at Strain 16.0 MPa
@Strain 0.26 %,
Temperature 23.0 °C
 28.6 MPa
@Strain 0.52 %,
Temperature 23.0 °C
 39.7 MPa
@Strain 0.78 %,
Temperature 23.0 °C
 49.3 MPa
@Strain 1.04 %,
Temperature 23.0 °C
 57.7 MPa
@Strain 1.3 %,
Temperature 23.0 °C
 64.1 MPa
@Strain 1.56 %,
Temperature 23.0 °C
 68.4 MPa
@Strain 1.82 %,
Temperature 23.0 °C
 71.1 MPa
@Strain 2.08 %,
Temperature 23.0 °C
 72.7 MPa
@Strain 2.34 %,
Temperature 23.0 °C
 74.3 MPa
@Strain 2.6 %,
Temperature 23.0 °C
Elongation at Break 3.5 %5mm/min; ISO 527-2/1A
 4.5 %
@Temperature 22.8 °C
ASTM D638
Tensile Modulus 4700 MPa1mm/min; ISO 527-2/1A
Flexural Strength 120 MPaISO 178
 17500 psi
@Temperature 22.8 °C
ASTM D790
Flexural Modulus 4400 MPaISO 178
 650000 psi
@Temperature 22.8 °C
ASTM D790
Izod Impact, Notched 0.900 ft-lb/in
@Temperature 22.8 °C
ASTM D256
Izod Impact, Notched (ISO) 5.60 kJ/m²ISO 180/1A
Charpy Impact Unnotched 21.0 kJ/m²ISO 179/1eU
 21.0 kJ/m²
@Temperature -30.0 °C
ISO 179/1eU
Charpy Impact, Notched 4.50 kJ/m²ISO 179/1eA
 4.50 kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+13 ohm-cmIEC 60093
 2.00e+16 ohm-cmASTM D257
Surface Resistance 1.00e+15 ohmIEC 60093
Dielectric Constant 3.0
@Frequency 1000 Hz
ASTM D150
 3.2
@Frequency 1e+6 Hz
ASTM D150
 3.4
@Frequency 1e+6 Hz
IEC 60250
 3.6
@Frequency 100 Hz
IEC 60250
Dielectric Strength 27.0 kV/mmIEC 60243-1
 540 V/milshort term; ASTM D149
Dissipation Factor 0.0033
@Frequency 100 Hz
IEC 60250
 0.010
@Frequency 1e+6 Hz
ASTM D150
 0.0165
@Frequency 1e+6 Hz
IEC 60250
Arc Resistance 78 secASTM D495
Comparative Tracking Index 225 VIEC 60112
 250 VASTM D3638
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 60.0 µm/m-°CISO 11359-2
Melting Point 225 °CISO 11357-1,-2,-3
 437 °FASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 210 °CISO 75-1, -2
 405 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 150 °CISO 75-1, -2
 315 °FASTM D648
Deflection Temperature at 8.0 MPa 55.0 °CISO 75-1, -2
Vicat Softening Point 200 °CB50 (50°C/h 50N); ISO 306
Glass Transition Temp, Tg 60.0 °CISO 11357-1,-2,-3
Flammability, UL94 V-0
 V-0
@Thickness 0.750 mm
 5VA
@Thickness 3.00 mm
Oxygen Index 30 %ISO 4589
 
Processing PropertiesOriginal ValueComments
Processing Temperature 20.0 - 50.0 °Chopper
 65.0 - 93.0 °Ccavity
Feed Temperature 230 - 240 °C
Zone 1 230 - 240 °C
Zone 2 235 - 250 °C
Zone 3 235 - 250 °C
Zone 4 240 - 255 °C
Die Temperature 250 - 255 °C
Melt Temperature 235 - 255 °C
 260 °CISO 294
Mold Temperature 82.0 °CISO 294
Injection Velocity 300 mm/secISO 294
Drying Temperature 120 - 130 °C
Dry Time 4 hour
Moisture Content 0.020 %Necessary low maximum
Injection Pressure 48.0 MPaISO 294
Hot-Working Temperature 250 - 260 °C
 
Descriptive Properties
Injection moldingYes
Injection speedmedium-fast
Melt volume rate (MVR), cm³/10min13
MVR test load, kg2.16
MVR test temperature, °C250
Processing conditions acc. ISO7792-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Celanex® 3100-2 PBT, 7.5% Glass Reinforced
Celanese Celanex® 3216 PBT, 15% Glass Reinforced
Celanese Celanex® 3216HR PBT, 15% Glass Reinforced
Celanese Celanex® 3316 PBT, 30% Glass Reinforced
Celanese Celanex® 3316HR PBT, 30% Glass Reinforced

PHCS037 / 123452

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.