MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Axiall 7055 Rigid PVC, Extrusion  (discontinued **)
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes: Georgia Gulf 7055 is a special purpose rigid PVC extrusion compound designed for applications requiring the following properties:
  • Weatherability
  • Chemical
  • Durability
  • Ease of Processing
  • Toughness

Information provided by Georgia Gulf

Georgia Gulf became Axiall Corporation, which was later acquired by Westlake Plastics. This specific grade is discontinued.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.43 g/ccASTM D-792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 106ASTM D-785
Hardness, Shore D 80ASTM D-2240
Tensile Strength, Yield 6000 psiASTM D-638
Tensile Modulus 374000 psiASTM D-638
Flexural Strength 11000 psiASTM D-790
Flexural Modulus 396000 psiASTM D-790
Izod Impact, Notched 16.0 ft-lb/in
@Thickness 6.35 mm,
Temperature 23.0 °C
ASTM D-256
 21.0 ft-lb/in
@Thickness 3.17 mm,
Temperature 23.0 °C
ASTM D-256
Tensile Impact Strength 80.0 ft-lb/in²ASTM D-1822
Dart Drop Total Energy 0.0920 ft-lb/mil23°C, C.125 Tup, Method A; ASTM D-4226
 0.290 ft-lb/milH.25 Tup, Method A; ASTM D-4226
 
Thermal PropertiesOriginal ValueComments
CTE, linear 36.0 µin/in-°F
@Temperature 20.0 °C
ASTM D-696
Deflection Temperature at 1.8 MPa (264 psi) 160 °FASTM D-648
 
Processing PropertiesOriginal ValueComments
Melt Temperature 360 °F
 
Descriptive Properties
Cell Classification14433233ASTM D-4216

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Alcoa 7055-T77511 Aluminum Extrusions
Aluminum 7055-T7751 Plate
Aluminum 7055-T77511 Extrusions
Alcoa 7055-T7751 Aluminum Plate
Aluminum 6063-T1

PGGUL410 / 41686

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.