MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Evonik TEGOPREN® 5851 Defoamer
Categories: Other Engineering Material

Material Notes: Product description: TEGOPREN® 5851 is a 100 % active defoamer based on organo-modified siloxanes.

Application: TEGOPREN® 5851 is used as an antifoam in multifunctional diesel fuel additive packages. TEGOPREN® 5851 is used for formulating stable, low foaming neat metal working fluids (MWF). TEGOPREN® 5851 is further used as lubricant in textile auxiliary formulation. TEGOPREN® 5851 can also be used in other lubricating oils (e.g. Transmission fluids and Industrial fluids). TEGOPREN® 5851 can either be blended directly into the oil or diesel fuel or used as part of an additive package.

Benefits:

  • TEGOPREN® 5851 provides good foam knock down and hold down properties.
  • TEGOPREN® 5851 is free of silicone oils. Therefore, it has no adverse effect on the finishing process (painting / electroplating etc.) of the treated parts.
  • TEGOPREN® 5851 has no negative impact on air release properties of lubricating oils.
  • TEGOPREN® 5851 is highly compatible.
  • In textile application TEGOPREN® 5851 reduces fiber and fiber metal friction in spin finish application.

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.045 - 1.065 g/cc
Viscosity 330 - 570 cP
Surface Tension 30 dynes/cm0.1% in water
 
Thermal PropertiesOriginal ValueComments
Flash Point >= 85.0 °C
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.447 - 1.452
 
Descriptive Properties
Appearanceliquid, colorless to pale straw
Cloud point61-67°C
Content100%Active matter

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Evonik TEGOPREN® 5852 Additive
Evonik TEGOPREN® 5885 Additive
Evonik TEGO® Antifoam 2290 Antifoam concentrate
Evonik TEGOPREN® 5847 Additive
Evonik TEGOPREN® 5863 Defoamer

PEVONIL596 / 196800

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.