MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LG Chemical LI968W Co-Extrusion ASA
Categories: Polymer; Thermoplastic; ASA Polymer; Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded

Material Notes: Description: Good Weatherability

Application: Window Profile, Siding, Rain Gutter

CAS: 26299-47-8

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.07 g/ccASTM D792
Maximum Moisture Content 0.010Extrusion Molding
Linear Mold Shrinkage, Flow 0.0040 - 0.0070 cm/cm
@Thickness 3.20 mm
ASTM D955
Melt Flow 12 g/10 min
@Load 10.0 kg,
Temperature 220 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 104ASTM D785
Tensile Strength, Yield 500 kg(f)/cm²
@Thickness 3.20 mm
50mm/min; ASTM D638
Elongation at Break 25 %
@Thickness 3.20 mm
50mm/min; ASTM D638
Elongation at Yield >= 6.0 %
@Thickness 3.20 mm
50mm/min; ASTM D638
Tensile Modulus 21000 kg(f)/cm²
@Thickness 3.20 mm
1mm/min; ASTM D638
Flexural Yield Strength 800 kg(f)/cm²
@Thickness 3.20 mm
15mm/min; ASTM D790
Flexural Modulus 23000 kg(f)/cm²
@Thickness 3.20 mm
15mm/min; ASTM D790
Izod Impact, Notched 4.00 kg-cm/cm
@Thickness 3.20 mm,
Temperature -30.0 °C
ASTM D256
 4.00 kg-cm/cm
@Thickness 6.40 mm,
Temperature -30.0 °C
ASTM D256
 14.0 kg-cm/cm
@Thickness 6.40 mm,
Temperature 23.0 °C
ASTM D256
 18.0 kg-cm/cm
@Thickness 3.20 mm,
Temperature 23.0 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 96.0 °C
@Thickness 6.40 mm
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 87.0 °C
@Thickness 6.40 mm
Unannealed; ASTM D648
Vicat Softening Point 95.0 °C
@Load 5.00 kg
50°C/h; ASTM D1525
Flammability, UL94 HB
@Thickness >=1.60 mm
 HB
@Thickness >=3.20 mm
 
Processing PropertiesOriginal ValueComments
Zone 1 190 - 200 °CExtrusion Molding
Zone 2 200 - 220 °CExtrusion Molding
Zone 3 210 - 230 °CExtrusion Molding
Zone 4 210 - 230 °CExtrusion Molding
Adapter Temperature 210 - 230 °CExtrusion Molding
Die Temperature 210 - 250 °CExtrusion Molding
Melt Temperature 200 - 230 °CExtrusion Molding
Roll Temperature 70.0 - 90.0 °CTop
 70.0 - 90.0 °CMiddle
 70.0 - 100 °CBottom
Drying Temperature 80.0 - 90.0 °CExtrusion Molding
Dry Time 2.00 - 3.00 hourExtrusion Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LG Chemical LI933 Co-Extrusion ASA
LG Chemical LI970 Co-Extrusion ASA
LG Chemical LI911 ASA
LG Chemical LI-913 ASA, Injection Molding, High Impact
LG Chemical LI968P ASA, Co-Extrusion

PLAY407 / 148417

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.