MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Super Oilite® Iron-Copper Bearing Alloy - SAE 863
Categories: Metal; Ferrous Metal

Material Notes: Super Oilite® is harder and of higher strength than Oilite bronze, although it has a lower speed rating in bearing applications. Oilite self-lubricating bearing products are made by a powder metallurgy process, allowing close control on the manufacturing process. They contain large interconnected pores to channel lubricants to the areas between shaft and bearing. Super Oilite is used in farm equipment, off road equipment, winches, sheaves, conveys, pulleys, etc.

Oilite® is the Registered US Trademark of Beemer Precision, Inc.

Key Words: ASTM B-439-95 GR. 4; MIL-B-5687D Type 2 GR 4
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 5.80 - 6.20 g/cc0.210 - 0.224 lb/in³
Porosity >= 15 %>= 15 %(% oil by volume)
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 152 MPa22000 psi
Elongation at Break 1.0 %1.0 %1 inch
Compressive Yield Strength 152 MPa22000 psi0.001 inch permanent set on 1.25 inch diameter by 1 inch long test specimen
Limiting Pressure Velocity <= 1.23 MPa-m/sec<= 35000 psi-ft/min
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 18 - 22 %18 - 22 %
Iron, Fe 76 - 82 %76 - 82 %As balance
Other, total <= 2.0 %<= 2.0 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Oilite® Bronze Bearing Alloy - SAE 841
Super Oilite® 16 Iron-Copper Bearing Alloy
Ampco Metal AMPCO® 18 Aluminum Bronze, Extruded and Drawn Rods, 12.7 - 25.4 mm.
High-Leaded Tin Bronze, UNS C93200, Copper Casting Alloy, Bearing Bronze SAE 660
Aluminum Bronze, UNS C95400, Copper Casting Alloy, TQ50 Temper

NOIL101 / 109233

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.