MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ITW Insulation XPS PIB Extruded Polystyrene Pipe Insulation Billet
Categories: Other Engineering Material

Material Notes: XPS PIB (extruded Polystyrene Pipe Insulation Billet) is a rigid thermoplastic foam manufactured by a proprietary extrusion process that forms a uniform, void-free, closed cell structure. This structure, along with the naturally water-repellent nature of the polystyrene resin, gives XPS PIB products high compressive strength, low friability and excellent resistance to water vapor and water absorption from freeze-thaw cycling. XPS PIB is non-dusting and non-irritating and is not a known food source for mold and mildew.

Applications: XPS PIB is used extensively in industrial and commercial piping applications. With a service temperature range of -297°F to 165°F (-183°C to 74°C), XPS PIB is a preferred material for low-temperature systems, both for minimizing heat gain and preventing surface condensation. XPS PIB maintains its key insulating properties in low-temperature applications and other environments with high humidity and high-moisture conditions. Typical applications for XPS PIB include:

  • ammonia refrigeration lines
  • freezer rooms
  • chilled water piping
  • transport pipelines
  • cold storage systems
  • refrigeration equipment
  • pharmaceutical plants
  • cryogenic systems

Information provided by ITW Insulation Systems

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.0260 g/ccASTM D1622
Water Absorption 1.0 %ASTM 272
 1.0 %ASTM C2842
 
Mechanical PropertiesOriginal ValueComments
Compressive Strength 20.0 psiASTM D1621
 
Thermal PropertiesOriginal ValueComments
CTE, linear 19.4 µm/m-°CASTM D696
Thermal Conductivity 0.0370 W/m-KAged 180 days; ASTM C518
Maximum Service Temperature, Air 74.0 °C
Minimum Service Temperature, Air -183 °C
Flame Spread Index <= 5.0
@Thickness <=102 mm
ASTM E84
 
Descriptive Properties
ColorBlue
Dimensional Stability+1% Changeat 70°C, 97% RH, 7 days, Volume, ASTM D2126
Surface Burning Characteristics165Smoke Developed, 4", ASTM E84
Water Vapor Permeability1.5 perm-inchASTM E96

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Elisto THERMOSTAR® XPS Mold Insulation Material
DuPont Styrofoam™ Polystyrene Rigid Foam Insulation
Arkema Appryl® 7280 Polypropylene - Polyethylene Copolymer
ITW Insulation TRYMER® Supercel Phenolic Insulation 2.5 lb/ft³ Density
Morgan Advanced Ceramics Vacupor® XPS-B2-S Porextherm

PITWZ015 / 187081

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.