MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Zell-Metall Engineering Plastics Zellamid 1500T (PEEK modified)  (discontinued **)
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK)

Material Notes: Zellamid® 1500 (Polyetheretherketone - PEEK, natural) is the registered trademark for Zell-Metall’s semi-crystalline high performance thermoplastic which exhibits a unique combination of high mechanical properties, temperature resistance and excellent chemical resistance, making it the most popular advanced plastics material.

Fields: Nuclear and Vacuum Technology, Aerospace Industry, Mechanical and Automotive Engineering, Conveyer Technology, Semiconductor Production, Electrical and Electronics, Wire and Cable, Oil Exploration, Chemical Processing Industry.

Besides of the standard grade for tribological applications also our Zellamid® 1500 T grade is available in black color, modified with 10% Carbonfibre, 10% PTFE and 10% Graphite.

Zellamid® 1500 T has an outstanding wear resistance and an even lower coefficient of friction as well as higher Pressure-Velocity capabilities.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.48 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 141 MPaISO 527; DIN 53455
Elongation at Break 2.0 %ISO 527; DIN 53455
Tensile Modulus 9.00 GPaISO 527; DIN 53452
 
Thermal PropertiesOriginal ValueComments
CTE, linear 22.0 µm/m-°C
@Temperature 20.0 °C
DIN 53752
Thermal Conductivity 0.240 W/m-KDIN 53612 Method A
Melting Point 340 °CISO 1218 Method A; DIN 53736
Maximum Service Temperature, Air 260 °C5000 hours; 50% Tensile Strength; IEC 216; DIN 53446
 300 °Ca few hours operation
Deflection Temperature at 1.8 MPa (264 psi) 293 °CISO 75; DIN 53461
Flammability, UL94 V-0
@Thickness 1.60 mm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Zell-Metall Engineering Plastics Zellamid 1500 (PEEK)
Zell-Metall Engineering Plastics Zellamid 1400 (PET)
VICTREX™ PEEK 90HMF40 Polyetheretherketone (PEEK), 40% Carbon Fiber Reinforced
VICTREX™ PEEK 450FC30 General Purpose
VICTREX™ PEEK 150FC30 Easy Flow

PZELL11 / 72940

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.