MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Borealis HE2590 High Density Polyethylene Compound for Crosslinked Pipes (Pex-C (Irradiation))
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Pipe Grade

Material Notes: HE2590 is a high molecular weight, high density polyethylene compound for crosslinkable pipes, especially designed for electron beam irradiation crosslinking. The stabilization is optimized for good processability, easy crosslinking as well as service at high temperatures.

Crosslinked pipes based on HE2590 are recommended for domestic hot and cold water supply, natural gas distribution, radiator connection, floor heating and industrial applications.

Former trade name for this product was BorPEX™.

Information provided by the Manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.944 g/ccBase Resin; ISO 1183
 0.946 g/ccCompound; ISO 1183
High Load Melt Index 8.5 g/10 min
@Load 21.6 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 2611 psiAt 50 mm/min; ISO 527-2
Elongation at Break >= 600 %ISO 527-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Borealis BorPEX™ ME2510 Medium Density Polyethylene Compound for Crosslinked Pipes (Pex-B (Silane))
Borealis BorPEX™ HE2557 Yellow High Density Polyethylene Compound for Crosslinked Pipes (Pex-A (Peroxide))
Borealis ME2592 Medium Density Polyethylene Compound for Crosslinked Pipes (Pex-C (Irradiation))
Borealis HE2595 Black High Density Polyethylene Compound for Crosslinked Pipes (Pex-C (Irradiation))
Borealis HE1878E High Density Polyethylene Powder for Crosslinked Pipes

PBOREA021 / 27328

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.