System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Cossa Polimeri ESTABLEND PSA 6600 PC / ASA Blend
Categories:
Polymer
;
Thermoplastic
;
ASA Polymer
;
Polycarbonate (PC)
;
Polycarbonate/ASA Alloy, Unreinforced
Material Notes:
Polycarbonate and acrylonitrile styrene acrylate blend
Good light resistance, good impact resistance, high heat resistance, excellent processability
Information provided by Cossa Polimeri S.r.l.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
1.13
g/cc
ASTM D 792
Linear Mold Shrinkage
0.0050
-
0.0070
cm/cm
ASTM D 955
Melt Flow
25
g/10 min
@Load 5.00 kg,
Temperature 260 °C
ASTM D 1238
Mechanical Properties
Original Value
Comments
Tensile Strength at Break
45.0
MPa
ASTM D 638
Tensile Strength, Yield
58.0
MPa
ASTM D 638
Elongation at Break
>= 50 %
ASTM D 638
Flexural Modulus
2400
MPa
ASTM D 790
Izod Impact, Notched
550
J/m
@Temperature 23.0 °C
ASTM D 256
Thermal Properties
Original Value
Comments
Vicat Softening Point
123
°C
@Load 5.00 kg
120°C/hr; ASTM D 1525
135
°C
@Load 0.999 kg
120°C/hr; ASTM D 1525
Flammability, UL94
HB
@Thickness 1.60 mm
HB
@Thickness 3.20 mm
Glow Wire Flammability Index
750
°C
I.E.C. 695-2-12
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Cossa Polimeri ESTABLEND PSA 7800 PC / ASA Blend
Covestro Bayblend® W85 HI PC ASA Blend
Techmer ES Plastiblend® PC/PBT IM 6600
Edinburg Plastics CYT605 PC/ASA
Chi Mei Wonderloy® PC-540 PC/ABS Alloy - Flame Retardant
PCOSSA931 / 156521
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.