MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
CeramTec 965 Toughened Alumina (Al2O3-ZrO2)
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: Hasselman Thermal Shock value is 270 K.

Data provided by CeramTec North America.

Key Words: Al2O3-ZrO2; Aluminum Oxide
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 4.20 g/cc
Water Absorption 0.00 %
 
Mechanical PropertiesOriginal ValueComments
Vickers Microhardness 1450HV 0.5
Tensile Strength, Ultimate 448 MPaACMA Test #4
Modulus of Elasticity 344 GPaUltrasonic
Flexural Strength 550 MPa20 x 40 mm
Compressive Strength 3586 MPaASTM C773-88
Poissons Ratio 0.26ASTM C-1 259-94
Fracture Toughness 7.20 MPa-m½
Shear Modulus 139 GPaUltrasonic
 
Thermal PropertiesOriginal ValueComments
CTE, linear 8.00 µm/m-°C
@Temperature 25.0 - 1001 °C
Specific Heat Capacity 0.700 J/g-°C
Thermal Conductivity 21.0 W/m-K
Maximum Service Temperature, Air 1400 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
CeramTec 950 Zirconia Toughened Alumina (ZTA), Al2O3•ZrO2
CeramTec Ziralit Zirconia Toughened Alumina (ZTA), Al2O3•ZrO2
CeramTec 977 Zirconia Toughened Alumina (ZTA), Al2O3•ZrO2
CeramTec Rubalit® A 1894 Alumina, 94%
CeramTec ATZ Alumina Toughened Zirconia, Dental Grade

CCERAC / 679

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.