MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Gromax PBT 4140-201D 40% Glass Fiber Filled
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled

Material Notes: Product Description: A glass fiber 40% reinforced injection molding grade.

Characteristics:

  • Excellent electrical property
  • Excellent temperature resistance, high heat distortion temperature
  • Excellent mechanic and chemical property
  • Excellent weatherability
  • Excellent wear property
  • Excellent moldability
  • High resistance to fuels, oil, fats and many solvents

    Information provided by Gromax Enterprises Corp.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.75 g/cc1.75 g/ccASTM D792
Moisture Absorption 0.0300 %
@Time 86400 sec
0.0300 %
@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage  0.0010 - 0.0040 cm/cm
@Thickness 1.60 mm
0.0010 - 0.0040 in/in
@Thickness 0.0630 in
horizontal; ASTM D955
 0.0070 - 0.013 cm/cm
@Thickness 1.60 mm
0.0070 - 0.013 in/in
@Thickness 0.0630 in
vertical; ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 9595ASTM D785
Tensile Strength 132 MPa19200 psiASTM D638
Elongation at Break 3.0 %3.0 %ASTM D638
Flexural Strength 180 MPa26100 psiASTM D790
Flexural Modulus 10.8 GPa1560 ksiASTM D790
Izod Impact, Notched >= 0.981 J/cm
@Thickness 6.35 mm
>= 1.84 ft-lb/in
@Thickness 0.250 in
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmASTM D257
Surface Resistance 1.00e+13 ohm1.00e+13 ohmASTM D257
Dielectric Constant 3.5
@Frequency 60 Hz
3.5
@Frequency 60 Hz
ASTM D150
Dielectric Strength 20.0 kV/mm
@Thickness 2.00 mm
508 kV/in
@Thickness 0.0787 in
ASTM D149
Dissipation Factor 0.0010
@Frequency 60 Hz
0.0010
@Frequency 60 Hz
ASTM D150
Arc Resistance 90 sec90 secASTM D495
 
Thermal PropertiesMetricEnglishComments
CTE, linear 30.0 µm/m-°C16.7 µin/in-°FASTM D696
Melting Point 225 °C437 °FDSC
Deflection Temperature at 0.46 MPa (66 psi) 210 °C410 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 190 °C374 °FASTM D648
Flammability, UL94 V-0
@Thickness 0.800 mm
V-0
@Thickness 0.0315 in
 
Processing PropertiesMetricEnglishComments
Processing Temperature 240 - 270 °C464 - 518 °F
Nozzle Temperature 260 - 270 °C500 - 518 °F
Mold Temperature 40.0 - 120 °C104 - 248 °Fsuitable temperature 60-80°C
Injection Pressure 50.0 - 120 MPa7250 - 17400 psi
Hold Pressure 30.0 - 80.0 MPa4350 - 11600 psi
Back Pressure 0.000 - 0.300 MPa0.000 - 43.5 psi
Screw Speed 60 - 120 rpm60 - 120 rpmto be chosen in such a way that plasticizing time is just within cooling time
 
Descriptive Properties
Injection Ratemiddle-fast

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Gromax CCP PBT 4815-NCB 15% Glass Fiber Filled
Gromax CCP PBT 4830-BK 30% Glass Fiber Filled
Gromax PBT 4115-104D 15% Glass Fiber Filled
Gromax PBT 4115-201D 15% Glass Fiber Filled
Gromax PBT 4130-104D 30% Glass Fiber Filled

PGROM036 / 147849

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.