MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Total PPR 7450HC Polypropylene, Film Extrusion Grade
Categories: Polymer; Film; Thermoplastic; Polypropylene (PP); Polypropylene, Film Grade

Material Notes: Random copolymer heat sealable film grade

Color - Low catalyst residuals in FINA 7450HC result in improved color stability.

Clarity/Impact - The random copolymer structure of FINA 7450HC improves its clarity and impact resistance over conventional homopolymer films.

Heat Sealable - The reduced melting point of FINA 7450HC makes it suitable as a heat seal layer for oriented films.

Slip/Antiblock - FINA 7450HC is formulated with a high level of antiblock additive for improved film handling.

FDA - FINA 7450HC complies with all applicable FDA regulations for food contact applications.

Recommended Applications - FINA 7450HC is recommended for use in either non-oriented cast film processes for manufacture of packaging films that require improved optical and impact properties or as a heat seal layer for oriented films.

Processing - FINA 7450HC resin processes on film extrusion equipment with typical melt temperatures of 450-525°F (232-274°C).

Data provided by the manuf

Total Petrochemicals acquired former Fina and Atofina plastics product lines.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ASTM D1505
Water Vapor Transmission 11.0 g/m²/day
@Temperature 37.8 °C
0.708 g/100 in²/day
@Temperature 100 °F
90% RH; thickness not specified; ASTM E96
Melt Flow 5.0 g/10 min5.0 g/10 minConditions not specified; ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Secant Modulus 0.550 GPa79.8 ksi1% Secant Modulus; Non-oriented Film; ASTM D882
Dart Drop 1.77 g/micron45.0 g/milF50; ASTM D 1709
Seal Strength >= 200 g/25 mm>= 200 g/inat 135°C, 15 psi pressure and 1 sec.
Film Tensile Strength at Break, MD 27.6 MPa4000 psiNon-oriented film; ASTM D882
 
Thermal PropertiesMetricEnglishComments
Melting Point 143 °C289 °FDSC
 
Optical PropertiesMetricEnglishComments
Haze 3.0 %3.0 %Non-oriented film; ASTM D1003
Gloss 80 %80 %45°; Non-oriented film; ASTM D2457
 
Processing PropertiesMetricEnglishComments
Melt Temperature 232 - 274 °C450 - 525 °Ffilm extrusion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Total PPH 3860X Polypropylene, Extrusion Grade
Total PPR 8473 Polypropylene, Film Extrusion Grade
Total 3868 Polypropylene, Extrusion Grade
Total PPR 8573 Polypropylene, Film Extrusion Grade
Braskem DS6D81 Polypropylene Random Copolymer

PFIN91 / 38421

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.