MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Morgan Advanced Ceramics Firemaster Board 350 Thermal Ceramic
Categories: Ceramic; Oxide

Material Notes: Alkaline Earth Silicate. Made exclusively from low bio-persistent alkaline earth silicate (AES) fibres, refractory fillers and a small amount of organic binders, this board is recommended for fire protection applications where lightweight, rigid panels are required. FireMaster® 350 board is available in thicknesses up to 50mm, is easy to cut and can be glued onto substrates for fast installation. The board is an excellent thermal insulator and is an ideal replacement for high density mineral wool saving weight and space.

Applications:

  • Compartment walls and ceilings from B15 standard upwards
  • Infill in fire doors and cladding systems
  • Floating floor systems in offshore and ship building industries.
  • Core material for fire rated decorative veneered panel systems
  • Ducting system

Information provided by Morgan Advanced Materials

Key Words: Thermal Ceramics
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.350 g/cc
Absorption Coefficient 0.080
@Frequency 125 Hz
test to BS EN 20354: 1993 Method
 0.33
@Frequency 250 Hz
test to BS EN 20354: 1993 Method
 0.63
@Frequency 500 Hz
test to BS EN 20354: 1993 Method
 0.71
@Frequency 1000 Hz
test to BS EN 20354: 1993 Method
 0.77
@Frequency 2000 Hz
test to BS EN 20354: 1993 Method
 0.89
@Frequency 4000 Hz
test to BS EN 20354: 1993 Method
 
Mechanical PropertiesOriginal ValueComments
Modulus of Rupture 0.00150 GPa
Compressive Strength 0.300 MPa10% reduction in thickness
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.0700 W/m-K
@Temperature 200 °C
ASTM C-201-68
 0.0800 W/m-K
@Temperature 300 °C
ASTM C-201-68
 0.0900 W/m-K
@Temperature 400 °C
ASTM C-201-68
 0.120 W/m-K
@Temperature 600 °C
ASTM C-201-68
 
Descriptive Properties
Colortan
Noise Reduction Coefficient0.61

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Morgan Advanced Ceramics Green Glass Paper Thermal Ceramic
Pyrotek Firefly 800 Roller & Furnace Cladding Material
Wacker Geniosil® GF 9 Silane
Unifrax FyreWrap® Marine Blanket Insulation
Thermal Ceramics V-19 Block Insulation

CMORF6071 / 202855

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.