MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Evonik Trogamid® BX9724 40% Glass Reinforced Nylon Blend  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6-3 (PA63)

Material Notes: Description: The TOGAMID® BX grades cover reinforced and non-reinforced blends based on PA 6-3-T and semi-crystalline polyamides. Non-reinforced blends are permanently transparent. Some blends have been developed in particular for manufacturing plastic-rubber composites. The special characteristics are:
  • high resistance to stress cracking
  • resistant to grease and fuels
  • good strength high hardness
  • very low mold shrinkage
  • very low tendency to warp
  • low moisture absorption
  • dimensionally stable even while absorbing water

The polyamide blends are especially suitable for the production of injection-molded parts subject to high thermal and mechanical stress. Thanks to their high stiffness moldings made from reinforced grades are appropriate for substituting cast metal parts, and are significantly lighter than these. Moldings exhibit outstanding surface qualities in spite of their high glass fiber content. TROGAMID® BX compounds can be combined with various rubber mixtures to produce plastic-rubber composite parts that are resistant to fuel and oil.

Specific Notes for this Material: Polymer blend consisting of amorphous and semi-crystalline polyamides, 40% glass fiber reinforced, with high tensile modulus for injection molding, dimensionally stable even while absorbing water; appropriate for substituting cast metal parts with plastic. Moldings exhibit outstanding surface qualities in spite of their high glass fiber content.

Information provided by degussa.

Evonik Industries is the successor company to Degussa.

Key Words: PA 6-3-T/XX, trimethyl hexamethylene diamine terephthalic acid
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.48 g/ccISO 1183
Viscosity Number 130 cm³/gISO 307
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 90ISO 868
Ball Indentation Hardness 262 MPaH30; ISO 2039-1
Tensile Strength at Break 220 MPa5 mm/min; ISO 527-1/2
Elongation at Break 3.2 %5 mm/min; ISO 527-1/2
 4.3 %5 mm/min, Outer fiber strain; ISO 178
Tensile Modulus 11.0 GPaISO 527-1/2
Flexural Strength 302 MPa5 mm/min, at 3.5% Strain; ISO 178
 342 MPa5 mm/min; ISO 178
Flexural Modulus 12.0 GPaISO 178
Charpy Impact Unnotched 8.00 J/cm²
@Temperature -30.0 °C
ISO 179/1eU
 8.70 J/cm²
@Temperature 0.000 °C
ISO 179/1eU
 9.60 J/cm²
@Temperature 23.0 °C
ISO 179/1eU
Charpy Impact, Notched 1.00 J/cm²
@Temperature -30.0 °C
ISO 179/1eA
 1.10 J/cm²
@Temperature 0.000 °C
ISO 179/1eA
 1.40 J/cm²
@Temperature 23.0 °C
ISO 179/1eA
Tensile Creep Modulus, 1 hour 9600 MPaISO 899-1
Tensile Creep Modulus, 1000 hours 5200 MPaISO 899-1
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cmIEC 60093
Surface Resistance >= 1.00e+13 ohmIEC 60093
 >= 1.00e+15 ohmSpec.; IEC 60093
Dielectric Constant 6.2
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 27.0 kV/mmK20/P50; IEC 60243-1
Dissipation Factor 0.025
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 600 VTest Solution A, 100 drops; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear 22.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
Longitudinal; ISO 11359
CTE, linear, Transverse to Flow 38.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
ISO 11359
Melting Point 260 °C10 K/min; DSC
Deflection Temperature at 0.46 MPa (66 psi) 230 °CISO 75-1/2
Vicat Softening Point 230 °C50N; ISO 306
Glass Transition Temp, Tg 93.0 °CTg, 10 K/min
Flammability, UL94 HB
@Thickness 0.800 mm
 HB
@Thickness 1.60 mm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Evonik Trogamid® BX9727 Nylon 6-3 Compound for Plastic-Rubber Composite
Evonik Trogamid® T-GF35 35% Glass Reinforced Amorphous Nylon
Evonik ROHACELL® 71 HERO Aircraft Grade Polymethacrylimide (PMI) Foam
Evonik Trogamid® BX7304 Nylon Blend
Covestro Bayblend® T88 GF-20 Polycarbonate + SAN Glass Filled Impact Grade

PHUK115 / 47249

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.