MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Westlake Plastics

Westlake Plastics Norylux™ Poly Phenylene Oxide
Categories: Polymer; Thermoplastic; Polyphenylene Ether/PPO

Material Notes: Norylux™ PPO modified Poly Phenylene Oxide is a high-strength, amorphous, engineering plastic with outstanding mechanical, thermal, and electrical properties. Low moisture absorption and low coefficient of thermal expansion make Norylux™ PPO one of the most dimensionally stable thermoplastics available. Norylux™ PPO is widely used for electrical housings and structural components since it has excellent insulating properties, flame resistance, strength and stiffness, and dimensional stability over a wide range of service temperatures. Norylux™ PPO is often selected for fluid handling applications since it has low moisture absorption and hydrolytic stability. Norylux™ PPO machines easily and may be fabricated into complex shapes with close tolerances. Norylux™ PPO is also easy to weld and glue, and it provides good adhesion to paints, inks, and other decorative coatings. Westlake Plastics extrudes and compression molds unfilled and flame-retardant products and compression molds glass reinforced and glass/mineral filled products.

Colors Available: Black

Attributes: Dimensional Stability; Good Contact; Impact Resistance; Dielectric Properties

Shapes: Compression Sheet; Extruded Sheet; Extruded Film; Extruded Rod. Available rod diamters are 0.5", 0.625", 0.75", 0.875", 1", 1.25", 1.375", 1.5" , 1.625", 1.75", 1.875", 2", 2.25", 2.5", 2.75", 3", 3.25", 3.5", 3.75", 4", 4.25", 4.5", 4.75", 5"

Information provided by Westlake Plastics Co.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.08 g/cc1.08 g/ccASTM D792
Moisture Absorption 0.0700 %0.0700 %ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 63.0 MPa9140 psiASTM D638
Elongation at Yield 25 %25 %ASTM D638
Flexural Yield Strength 99.0 MPa14400 psiASTM D790
Flexural Modulus 2.55 GPa370 ksiASTM D790
Izod Impact, Notched 0.990 J/cm1.85 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 123 °C253 °FASTM D648
 
Descriptive Properties
Compression Sheet Sizing120" Length by 48" Width0.25", 0.375", 0.5", 0.75", 1", 1.25", 1.5", 1.75", 2", 2.25", 2.5", 2.75", 3", 3.25", 3.5", 3.75", 4"
 120" Length by 60" Width0.25", 0.375", 0.5", 0.75", 1", 1.25", 1.5", 1.75", 2", 2.25", 2.5", 2.75", 3", 3.25", 3.5", 3.75", 4"
 48" Length by 24" Width0.25", 0.375", 0.5", 0.75", 1", 1.25", 1.5", 1.75", 2", 2.25", 2.5", 2.75", 3", 3.25", 3.5", 3.75", 4", 4.25", 4.5", 4.75", 5", 5.25", 5.5", 5.75", 6"
 96" Length by 48" Width0.25", 0.375", 0.5", 0.75", 1", 1.25", 1.5", 1.75", 2", 2.25", 2.5", 2.75", 3", 3.25", 3.5", 3.75", 4", 4.25", 4.5", 4.75", 5", 5.25", 5.5", 5.75", 6"
Extruded Sheet Sizing96" Length by 48" Width0.03", 0.035", 0.06", 0.062", 0.08", 0.09", 0.95", 0.125", 0.1875", 0.25"
Film Sizing26" Width0.002", 0.003", 0.004", 0.005", 0.01" 0.02"
Rod Sizing48" Length
 96" Length

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PWEST884 / 297286

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.