MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Ravago Manufacturing Americas Hylon® N1000STHLUV2 HF Nylon 6/6  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Heat Stabilized

Material Notes:
  • Available in North America
  • Additive: Heat Stabilizer, Lubricant and UV Stabilizer
  • Features: Good Toughness, Lubricated, Heat Stabilized and High Flow
  • RoHS Compliant
  • Auto Specifications: GM GMP.PA66.074 Color: Black, GM GMP.PA66.078 Color: Black, GM GMP.PA66.089 Color: Black
  • Form: Pellets
  • Processing Method: Injection Molding

Information provided by Ravago.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.09 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.017 - 0.021 in/in
@Thickness 3.17 mm
ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 7800 psiASTM D638
Elongation at Break 50 %ASTM D638
Flexural Strength 10200 psiASTM D790
Flexural Modulus 265000 psiASTM D790
Izod Impact, Notched 16.0 ft-lb/inASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 144 °FUnannealed; ASTM D648
Flammability, UL94 HB
@Thickness 0.787 mm
 
Processing PropertiesOriginal ValueComments
Melt Temperature 510 - 530 °F
Mold Temperature 150 - 180 °F
Drying Temperature 165 °F
@Time 7200 - 14400 sec
Moisture Content <= 0.18 %Suggested Maximum
Back Pressure 20.0 - 50.0 psi
Screw Speed 40 - 120 rpm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ravago Manufacturing Americas Hylon® N1000STHL UV2 Nylon 6/6
Ravago Manufacturing Americas Hylon® N1000THLUV2 Polyamide 66
Ravago Manufacturing Americas Hylon® N1000THLHF2 Nylon 6/6
Ravago Manufacturing Americas Hylon® N1000 Nylon 6/6 (DAM)
Ravago Manufacturing Americas Hylon® N1000 Nylon 6/6 (Cond)

PENTA107c / 142973

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.