MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BASF Ultramid® T 4381 LDS 10/25% Glass/Mineral Filled PA6/6T (Conditioned)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Glass/Mineral Reinforced

Material Notes: Description: Ultramid® T 4381 LDS is a semi-crystalline, partially aromatic high temperature polyamide (PA6/6T) for laser direct structuring (LPKFLDS®). As the material is reinforced with 10% fiberglass and 25% mineral filling, high-strength mechatronic plastic parts can be manufactured efficiently, quickly and flexibly with LDS. The innovative material offers a broad processing window for optimal results regarding: laser activation, metallization, adhesion of the conductors. Ultramid T 4381 LDS is based on Ultramid T and offers an ideal combination of high melting temperature, good processability and low water absorption. This specialty from BASF’s engineering plastics is already being used in electrical engineering and automotive construction, especially where high heat distortion temperature is required.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.52 g/ccISO 1183
Water Absorption 4.2 - 5.2 %ISO 62
Moisture Absorption at Equilibrium 0.80 - 1.2 %50% RH; ISO 62
Viscosity Measurement 130ISO 307
Linear Mold Shrinkage 0.0047 cm/cm
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 3.00e+12 ohm-cmIEC 60093
Dielectric Constant 4.2
@Frequency 1e+6 Hz
IEC 60250
Dissipation Factor 0.038
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 600 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
Melting Point 295 °CISO 3146
Deflection Temperature at 0.46 MPa (66 psi) 265 °CISO 75-2
 
Processing PropertiesOriginal ValueComments
Melt Temperature 310 - 330 °CInjection molding/Extrusion
Mold Temperature 100 - 140 °CInjection molding
 
Descriptive Properties
ColorBlack
Commercial StatusEurope

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Ultramid® T 4381 LDS 10/25% Glass/Mineral Filled PA6/6T (Dry)
EMS-Grivory Grivory® HT XE 4027 black 9916 PA*-GF30
Kingfa LONOY 2100 LT PC/PET Alloy
Mitsubishi Xantar® LDS 3760 Polycarbonate
Magnesium AZ91D-F, Cast

PBASG0353 / 131986

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.