MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Arla MULTICLEAR® RPC PC Sheet
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Optical Grade

Material Notes: MULTICLEAR® RPC is a polycarbonate sheet extruded primarily from regrind polycarbonate. With MULTICLEAR® RPC you will get a product with high impact strength and high temperature resistance. MULTICLEAR® RPC is suitable for outdoor applications. The RPC sheet can bet protected against UV on the top side. To widen the use the RPC sheet can be offered in black multiwall structure with one co-extruded side. The product can also be produced with BOX 2W, BOX 3W and STRONG structures. Multiclear RPC can be colored and available in varying thicknesses.

Benefits: Lower costs than standard polycarbonate materials; More than 10 times the impact strength of PMMA; More than 4 times the impact strength of PVC; One side UV as standard

Application: Internal partitions, soundproofing, hospital room privacy partitions, farmhouse partitions and roofing, furniture parts. Ideal for cladding, transport boxes and packaging.

Information provided by Arla Plast.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.20 g/ccISO 1183
Moisture Absorption 0.150 %
@Time 86400 sec
50% RH; ISO 62
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 70ISO 2039-2
Tensile Strength at Break 70.0 MPaISO 527
Tensile Strength, Yield 63.0 MPaISO 527
Elongation at Break 110 %ISO 527
Elongation at Yield 6.0 %ISO 527
Modulus of Elasticity 2.30 GPaISO 527
Flexural Modulus 2300 MPaISO 178
Izod Impact, Notched (ISO) 10.0 kJ/m²
@Temperature -30.0 °C
ISO 180/1A
 65.0 kJ/m²
@Temperature 23.0 °C
ISO 180/1A
Charpy Impact Unnotched NB
@Temperature 23.0 °C
ISO 179/2D
 NB
@Temperature -40.0 °C
ISO 179/2D
 
Thermal PropertiesOriginal ValueComments
CTE, linear 70.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
Specific Heat Capacity 0.00117 J/g-°C
Thermal Conductivity 0.210 W/m-KDIN 52612
Deflection Temperature at 0.46 MPa (66 psi) 142 °CISO 75
Deflection Temperature at 1.8 MPa (264 psi) 132 °CISO 75
Vicat Softening Point 148 °CB 50; ISO 306
 149 °CB 120; ISO 306
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.586ISO 489

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PARLA924 / 301102

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.