MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BASF Lupranate® M20 Isocyanate
Categories: Fluid

Material Notes: Description: Lupranate® M20 Isocyanate is a polymeric MDI with a functionality of approximately 2.7. Lupranate M20 Isocyanate can be used for the production of rigid insulation foams by molding, spraying, and frothing. It is also used for rigid and semi-flexible integral skin foams, adhesives, sealants, elastomers, and high-resiliency flexible foams. In low catalyzed rigid urethane formulations, the foam rise time can be lengthened by 20-30%. The slower reactivity can be advantageous in applications such as large rigid foam panels or molded flexible foams.

Information provided by BASF

Key Words: Polymethylene Polyphenylpolyisocyanate
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.23 g/cc
Viscosity 200 cP
Vapor Pressure 2.67e-7 bar
@Temperature 25.0 °C
 
Thermal PropertiesOriginal ValueComments
Boiling Point >= 190 °C
@Pressure 0.000667 MPa
Flash Point 200 °C
 
Descriptive Properties
ColorDark Brown
CompositionHydrolyzable Chlorine0.00035
 NCO content0.315

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Lupranate® M20SB Isocyanate
BASF Lupranate® 281 Isocyanate
BASF Lupranate® 277 Isocyanate
BASF Lupranate® 5010 Isocyanate
BASF Lupranate® 8020 Isocyanate

PBASG0692 / 132325

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.