MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Evonik DYNACOLL® AC 1520 Polyacrylate
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Adhesives, Sealants, and Coatings

Material Notes: Polyacrylates: With its DYNACOLL® AC product range Evonik offers acrylics for one-component moisture curable hot melt adhesives. Acrylics for adhesives are bead polymers made of methyl methacrylate and n-butyl methacrylate which are mainly used to modify reactive hot melts for flat lamination applications. Various DYNACOLL® AC grades with tailored glass transition temperature and molecular weight are available. They also differ according to their acid and hydroxyl functionality. DYNACOLL® AC polyacrylates are supplied as beads in bags of 25 kg.

Your benefits

  • DYNACOLL® AC provides outstanding quality and flow properties
  • DYNACOLL® AC modified reactive hot melts provide
  • low viscosity
  • very long open time
  • aggressive tack
  • high creep resistance directly after bonding
Applications: DYNACOLL® AC grades are mainly used to modify reactive hot melts for flat lamination purposes. Typical areas of application are:
  • Sandwich composites: of aluminium, FRP panels, foam or wood-based substrates e. g. for recreational vehicals
  • Honeycomb structures: e.g. for door manufacturing
  • Foil laminated particleboard: e.g. for furniture
  • Medium density fiberboard panels: e.g. for furniture
Flat lamination applications require long open times to permit long handling times needed to bond huge panels or sandwich composites. On the other hand, initial strength has to be very high to hold the bonded parts in place without any further mechanical fixation.

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity Number 19 cm³/gISO 1628-1
Molecular Weight 35000 g/molDIN 55627-1
Melt Flow 500 g/10 min
@Load 2.20 kg,
Temperature 190 °C
DIN ISO 1133
 
Chemical PropertiesOriginal ValueComments
Total Acid Number 8.5[mg KOH/g]; DIN EN ISO 2114
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg 48.0 °CISO 11357-1
Ring & Ball Softening Point 135 °CDIN ISO 4625

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Evonik DYNACOLL® AC 1920 Polyacrylate
Evonik DYNACOLL® AC 1750 Polyacrylate
Evonik DYNACOLL® AC 1631 Polyacrylate
Evonik DYNACOLL® AC 1630 Polyacrylate
Evonik DYNACOLL® AC 1620 Polyacrylate

PEVONIL105 / 196309

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.