MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Alcoa KAMA 7120 Calcium Carbonate Filled Homopolymer Polypropylene (PP)  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Capabilities
  • Gauge: .015” to .060” (381 to 1524µm)
  • Width: 12” to 55” (305 to 1397mm)
  • Core size: 6” standard, also available in 3” and 8”
  • Roll O.D.: 29” standard, available up to 40”
  • Silicone coated available
  • Custom colors available

Properties

  • Excellent stiffness
  • Mineral filled
  • Improved processability
  • Wide range of temperature use
  • Excellent for microwaveable applications
  • FDA compliant

Information provided by Alcoa Kama Co.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.24 g/cc
Thickness 15.0 - 60.0 mil
Linear Mold Shrinkage 0.012 - 0.014 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 3200 - 3800 psiASTM D638
Elongation at Break 50 - 150 %ASTM D638
Flexural Modulus 230000 - 270000 psiASTM D790
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 230 °F
Minimum Service Temperature, Air -10.0 °F
 
Optical PropertiesOriginal ValueComments
Haze <= 12 %
 
Processing PropertiesOriginal ValueComments
Processing Temperature 280 - 360 °FThermoforming Temp
 
Compliance PropertiesOriginal ValueComments
FDA Yes
 
Descriptive Properties
Resistance to AcidGood to Excellent
Resistance to AlcoholsGood to Excellent
Resistance to AlkalisGood
Resistance to Fat, Grease, and OilGood to Excellent
Resistance to Hydrocarbon SolventsGood
Resistance to Strong OxidizersFair to Good
Yield, in²/lb/mil23800

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Excalibar ExCal® CW 325 Calcium Carbonate CaCO3 Powder
CIMBAR RiverCal™ 8107 & 8107C Calcium Carbonate (CaCO3)
CIMBAR Crescent 12 Calcium Carbonate (CaCO3), Fine Powder
Calcium Carbonate, Calcite (CaCO3)
Buckeye Polymers BP RPP 2011 C Polypropylene, 20% Mineral Filled

PKAMA33 / 48689

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.