MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LyondellBasell Astryn EPKT25M Polypropylene Copolymer, Mineral Filled  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes:
Key Features: conventional melt flow, very high modulus, mineral-filled polypropylene copolymer, high rigidity, good impact resistance, good dimensional stability, low fogging

Applications: glove box close-outs

Description: Astryn EPKT25M conventional melt flow, mineral-filled polypropylene copolymer has a good balance of stiffness, impact resistance and dimensional stability. It was designed for a variety of non-cosmetic automotive interior applications.

Information provided by Montell Polyolefins.

LyondellBasell is the successor company to Montell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.21 g/ccISO 1183
Linear Mold Shrinkage 0.0090 cm/cmISO 2577
Melt Flow 6.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 90ISO 2039-2
Hardness, Shore D 67ISO 868
Tensile Strength, Yield 26.0 MPaISO R527
Elongation at Yield 4.0 %ISO R527
Flexural Modulus 3.30 GPaISO 178
Izod Impact, Notched 3.20 J/cm
@Temperature 23.0 °C
ISO 180
 
Thermal PropertiesOriginal ValueComments
CTE, linear 30.0 µm/m-°C
@Temperature -30.0 - 30.0 °C
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 131 °CISO 75

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Borealis ME212U Polypropylene Compound, Mineral Filled
Polyplastic Armlen® PP MD 40-4HS-901 Polypropylene, 40% Mineral Filled
Momentive Performance Materials HCT-40 Titanium Diboride (TiB2) Powder
Polykemi AB POLYfill PPC T25020 UV Polypropylene Copolymer, Mineral Reinforced
Phillips Sumika Marlex® AGN-380 Polypropylene Impact Copolymer, Heat-stabilized, nucleated

PMO405 / 53624

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.