MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Zell-Metall Engineering Plastics Zellamid 900 (POM-C) at 50% RH
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Unreinforced

Material Notes: Zellamid® 900 is the registered trademark of Zell-Metall’s high molecular weight Acetal resin.

Acetal (POM) is noted for its high mechanical strength, heat resistance and good antifriction properties. As water absorption is almost nil dimensional accuracy and stability is higher than that of nylons. Physical properties remain unchanged in various environments. This material is manufactured in natural - Zellamid® 900 and black color - Zellamid® 900 SW, using Copolymer resin. Homopolymer Acetal is available on special request. Typical applications are gears, levers, springs, snap connectors, cam switches, clamps, pump components, mud handling equipment, electronic and office machines . Acetal lends itself also to all submerged applications.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.41 - 1.43 g/ccDry Density
Moisture Absorption at Equilibrium 0.20 %50% RH; ISO 1110; DIN 53714
Water Absorption at Saturation 0.25 %23°C; ISO 62; DIN 53495
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 115 MPaH 358/30; ISO 2039; DIN 53456
Tensile Strength at Break 70.0 MPaISO 527; DIN 53455
Elongation at Break 40 %ISO 527; DIN 53455
Tensile Modulus 3.00 GPaISO 527; DIN 53452
Charpy Impact Unnotched 80.0 J/cm² - NB
@Temperature -40.0 °C
ISO 179; DIN 53453
 NB
@Temperature 23.0 °C
ISO 179; DIN 53453
 
Electrical PropertiesOriginal ValueComments
Comparative Tracking Index >= 600 VKB Method; IEC 112; DIN 53480
 
Thermal PropertiesOriginal ValueComments
Melting Point 164 - 168 °CISO 1218 Method A; DIN 53736
Maximum Service Temperature, Air 100 °C20,000 hours; 50% Tensile Strength; IEC 216; DIN 53446
Flammability, UL94 HB
@Thickness 1.60 mm
 
Descriptive Properties
Time yield limit14 MPa23°C, s1/1000; ISO.899 DIN.53444

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Kolon Kocetal® WH702 Reinforced Grade Acetal Copolymer
Zell-Metall Engineering Plastics Zellamid 900 (POM-C)
Omnia Plastica Arnite Omnialite POM c Acetal Copolymer
Omnia Plastica Akulon® POM h Acetal Homopolymer
Kolon Kocetal® VT701 Modified Grade Acetal Copolymer

PZELL06 / 72935

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.