MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Haynes Waspaloy™ alloy, sheet
Categories: Metal; Nonferrous Metal; Nickel Alloy; Superalloy

Material Notes: Age-hardenable superalloy with very good strength at temperatures up 980°C (1800°F), can be cold-formed in the annealed condition, may also be hot formed at 1040°C (1900°F) and above, good resistance to gas turbine combustion gas environments at temperatures up to 870°C (1600°F). Widely used as a wrought material for forged and fabricated gas turbine and aerospace components.

Tensile properties reported after heat treatment per AMS 5544: 1975°F (1080°C)/30 min./WQ + 1825°F (995°C)/2 hr./AC + 1550°F (845°C)/4 hr./AC + 1400°F (760°C)/16hr./AC

Data provided by the manufacturer, Haynes International, Inc.

Key Words: AMS 5544
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 8.20 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 1335 MPa
 83.0 MPa
@Temperature 1095 °C
 220 MPa
@Temperature 980 °C
 545 MPa
@Temperature 870 °C
 970 MPa
@Temperature 760 °C
 1195 MPa
@Temperature 650 °C
Tensile Strength, Yield 910 MPa
@Strain 0.2 %
 41.0 MPa
@Strain 0.2 %,
Temperature 1095 °C
 135 MPa
@Strain 0.2 %,
Temperature 980 °C
 415 MPa
@Strain 0.2 %,
Temperature 870 °C
 770 MPa
@Strain 0.2 %,
Temperature 650 °C
 770 MPa
@Strain 0.2 %,
Temperature 760 °C
Elongation at Break 26.6 %in 51 mm
 12 %
@Temperature 760 °C
in 51 mm
 12 %
@Temperature 870 °C
in 51 mm
 19.4 %
@Temperature 980 °C
in 51 mm
 20.8 %
@Temperature 650 °C
in 51 mm
 36.8 %
@Temperature 1095 °C
in 51 mm
Modulus of Elasticity 146 GPa
@Temperature 1000 °C
 155 GPa
@Temperature 900 °C
 164 GPa
@Temperature 800 °C
 172 GPa
@Temperature 700 °C
 180 GPa
@Temperature 600 °C
 192 GPa
@Temperature 400 °C
 204 GPa
@Temperature 200 °C
 213 GPa
@Temperature 20.0 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 13.9 µm/m-°C
@Temperature 20.0 - 500 °C
 14.3 µm/m-°C
@Temperature 20.0 - 600 °C
 14.8 µm/m-°C
@Temperature 20.0 - 700 °C
 15.4 µm/m-°C
@Temperature 20.0 - 800 °C
 16.4 µm/m-°C
@Temperature 20.0 - 900 °C
 17.8 µm/m-°C
@Temperature 20.0 - 1000 °C
Thermal Conductivity 12.6 W/m-K
@Temperature 200 °C
 15.7 W/m-K
@Temperature 400 °C
 19.1 W/m-K
@Temperature 600 °C
 20.9 W/m-K
@Temperature 700 °C
 22.7 W/m-K
@Temperature 800 °C
 24.5 W/m-K
@Temperature 900 °C
Melting Point 1330 - 1360 °C
Solidus 1330 °C
Liquidus 1360 °C
Maximum Service Temperature, Air 980 °Cstrength retained
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 1.5 %
Boron, B 0.0060 %
Carbon, C 0.080 %
Chromium, Cr 19 %
Cobalt, Co 13.5 %
Iron, Fe <= 2.0 %
Manganese, Mn <= 0.10 %
Molybdenum, Mo 4.3 %
Nickel, Ni 56 %As Remainder
Silicon, Si <= 0.15 %
Titanium, Ti 3.0 %
Zirconium, Zr 0.050 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ATI Allvac® WASPALOY® Nickel Superalloy, Heat Treatment: 1010°C (1850°F) + Age
MetalTek WASPALOY® Centri-Vac Nickel Cobalt Based Alloy
Waspaloy A Nickel Superalloy (UNS N07001)
Waspaloy B Nickel Superalloy
ATI Allvac® Rene 41® Nickel Superalloy, Heat Treatment: 1079°C (1975°F) + Age

NHWASA / 17373

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.