MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SABIC LEXAN™ Copolymer EXL9414 Polycarbonate (PC) (Americas)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: LEXAN EXL9414 polycarbonate (PC) siloxane copolymer resin is a medium flow, non-chlorinated, non-brominated flame retardant opaque injection molding (IM) grade. This resin offers low temperature ductility, thin wall flame retardant capability, and in combination with excellent processability and release with opportunities for shorter IM cycle times compared to standard PC. LEXAN EXL9414 resin is a product available in wide range of opaque colors and may be an excellent candidate for a wide variety of applications, especially the housing of fast-charging mobile phones.

Features: High Impact Resistance

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.19 g/ccASTM D792
Density 1.19 g/ccISO 1183
Moisture Absorption 0.0200 %Injection Molding
Viscosity 10 cP
@Load 1.20 kg,
Temperature 300 °C
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0040 - 0.0080 cm/cm
@Thickness 3.20 mm
SABIC method
Linear Mold Shrinkage, Transverse 0.0040 - 0.0080 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 11.5 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell L 83ASTM D785
Hardness, Rockwell R 117ASTM D785
Tensile Strength at Break 60.0 MPa50 mm/min; ISO 527
 62.0 MPa50 mm/min; ASTM D638
Tensile Strength, Yield 56.0 MPa50 mm/min; ASTM D638
 57.0 MPa50 mm/min; ISO 527
Elongation at Break 106 %50 mm/min; ISO 527
 107 %50 mm/min; ASTM D638
Elongation at Yield 5.6 %50 mm/min; ISO 527
 5.8 %50 mm/min; ASTM D638
Tensile Modulus 2110 MPa50 mm/min; ASTM D638
 2140 MPa1 mm/min; ISO 527
Flexural Strength 86.0 MPayield, 2 mm/min; ISO 178
 88.0 MPayld, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2180 MPa2 mm/min; ISO 178
 2190 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched 880 JASTM D256
 660 J
@Temperature -30.0 °C
ASTM D256
Izod Impact, Notched (ISO) 69.0 kJ/m²80*10*3; ISO 180/1A
 46.0 kJ/m²
@Temperature -30.0 °C
80*10*3; ISO 180/1A
Charpy Impact, Notched 75.0 kJ/m²Edgew 80*10*3 sp=62mm; ISO 179/1eA
 29.0 kJ/m²
@Temperature -30.0 °C
Edgew 80*10*3 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 67.0 JASTM D3763
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+16 ohm-cmASTM D257
Surface Resistance >= 1.00e+16 ohmASTM D257
Dielectric Constant 2.78
@Frequency 1.10e+9 Hz
ASTM ES 7-83
Dielectric Strength 13.0 kV/mm
@Thickness 3.20 mm
in oil; ASTM D149
Dissipation Factor 0.0060
@Frequency 1.10e+9 Hz
ASTM ES 7-83
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 69.1 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 74.2 µm/m-°C
@Temperature 23.0 - 80.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 72.7 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 76.4 µm/m-°C
@Temperature 23.0 - 80.0 °C
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 131 °CEdgew 120*10*4 sp=100mm; ISO 75/Be
 134 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 117 °CEdgew 120*10*4 sp=100mm; ISO 75/Ae
 118 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Vicat Softening Point 136 °CRate B/50; ISO 306
 138 °CRate B/120; ISO 306
UL RTI, Electrical 80.0 °CUL 746B
UL RTI, Mechanical with Impact 80.0 °CUL 746B
UL RTI, Mechanical without Impact 80.0 °CUL 746B
Flammability, UL94 V-2
@Thickness >=0.500 mm
UL 94
 V-1
@Thickness >=0.800 mm
UL 94
 V-0
@Thickness >=1.00 mm
UL 94
 5VB
@Thickness >=1.50 mm
UL 94
 5VA
@Thickness >=3.10 mm
UL 94
Oxygen Index 39 %ISO 4589
Glow Wire Flammability Index 960 °C
@Thickness 1.00 mm
IEC 60695-2-12
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 290 - 310 °C
Zone 2 280 - 305 °C
Zone 3 295 - 315 °C
Melt Temperature 295 - 315 °CInjection Molding
Mold Temperature 70.0 - 95.0 °C
Drying Temperature 120 °CInjection Molding
Dry Time 3.00 - 4.00 hourInjection Molding
 48.0 hourCumulative; Injection Molding
Back Pressure 0.300 - 0.700 MPa
Shot Size 40 - 60 %
Vent Depth 0.00250 - 0.00760 cm
Screw Speed 40 - 70 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH80239 / 288186

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.