MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ExxonMobil Santoprene® 8221-60 Thermoplastic Rubber
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Elastomer, Melt-Processible Rubber

Material Notes: A soft, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range of applications. This grade of Santoprene TPV is shear-dependent and can be processed on conventional thermoplastics equipment for injection molding or blow molding. It is polyolefin based and completely recyclable.

Key Features:

  • UL listed: file #QMFZ2.E80017, Plastics - Component; file #QMFZ8.E80017, Plastics Certified For Canada - Component.
  • Neutral, easy coloring formulation.
  • Used in sealing applications.
  • EU and China RoHS compliant.
Applications:
  • Industrial - Architectural and Construction
Uses:
  • Construction Applications
  • Glazing
  • Expansion Joint
  • Outdoor Applications
Processing Method: Blow Molding, Extrusion Blow Molding, Injection Blow Molding, Injection Molding and Multi Injection Molding

Availability: Africa & Middle East, Europe, North America, Asia Pacific, Latin America and South America

Information provided by ExxonMobil Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.950 g/ccASTM D792
Maximum Moisture Content 0.080
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 642 mm, 15 sec; ISO 868
Tensile Strength at Break 827 psiAcross flow; ASTM D412
Tensile Stress at Strain 319 psi
@Strain 100 %
Across flow; ASTM D412
Elongation at Break 470 %Across flow; ASTM D412
Compression Set 32 %
@Temperature 70.0 °C,
Time 79200 sec
ASTM D395B
 60 %
@Temperature 125 °C,
Time 252000 sec
ASTM D395B
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 2.3
@Thickness 2.01 mm
ASTM D150
Dielectric Strength 790 V/mil
@Thickness 2.03 mm
ASTM D149
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature -81.0 °FASTM D746
UL RTI, Electrical 100 °CUL 746
UL RTI, Mechanical with Impact 85.0 °CUL 746
Flammability, UL94 HB
@Thickness 1.10 mm
 HB
@Thickness 3.00 mm
 
Processing PropertiesOriginal ValueComments
Processing Temperature 175 - 230 °C
Rear Barrel Temperature 177 - 191 °C
Middle Barrel Temperature 179 - 193 °C
Front Barrel Temperature 185 - 199 °C
Nozzle Temperature 185 - 210 °C
Die Temperature 177 - 216 °CExtrusion
Melt Temperature 143 - 216 °CProcessing
 179 - 216 °CExtrusion
Mold Temperature 23.9 - 51.7 °C
Drying Temperature 82.0 °C
Dry Time 3 hour
Back Pressure 0.345 - 0.689 MPa
Clamp Pressure 41.0 - 69.0 MPa
Vent Depth 0.00100 in
Cushion 0.125 - 0.250 in
Screw Speed 100 - 200 rpm
 
Descriptive Properties
Injection RateFast
Max Regrind20%
Screw Compression Ratio2:1 - 2.5:1
Screw L/D Ratio16:1 - 20:1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ExxonMobil Santoprene® 101-64 Thermoplastic Elastomer
A. Schulman Alcryn® 1060 BK Melt Processable Rubber
A. Schulman DuraGrip™ DGR 6160 NC Thermoplastic Elastomer (TPE)
A. Schulman DuraGrip™ DGR 6060 NC Thermoplastic Elastomer (TPE)
A. Schulman Alcryn® 2060 NC Melt Processable Rubber

PADW160 / 22878

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.