MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Chemtotal Mica Micronized Mica
Categories: Ceramic; Oxide; Other Engineering Material

Material Notes: Micronized Mica for paints and coatings, cosmetics, rubber, plastic and polymer formulations.

Micronized Muscovite Mica is pigment extender in various paints and coatings & regarded tough, flexible and transparent.

Mica is an antifriction, antifouling, antisettling, anticorrosive, antitarmish and antisiege agent. The over lapping layers of mica platelets form a tough shield that improves paint integrity and durability.

Mica acts as a reinforcing pigment to reduce cracking, peeling and checking in the dry film and prevents shrinkage and sheering of the paint. When a paint starts to fall, mica holds it together sufficiently to keep it away from cissing, curtaining and prevents microscopic ruptures in the paint films.

Mica particles brighten the tone of the colored pigments, at the same time, transmit and reflect light resulting in proven decorative effects and design. It increases the gloss of paint more effectively than spherical or irregularly shaped filler particles of an equivalent size product. Mica also optimize the effect of other pigments by ensuring that the pigment particles are evenly spaced in the dried paint film.

Mica is widely used in Aluminum, automotive, anti corrosive, cement, emulsion, synthetic, water, fire resistant, marine, road marking, textured, traffic paints.

Mica also finds applications in cosmetic, paint and coatings, rubber, electronics, plastics and polymers, refractory, insulation, metallurgical formulations.

Information provided by Chemtotal

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Component Elements PropertiesOriginal ValueComments
Al2O3 26.98 %
CaO 0.425 %
Fe2O3 1.35 %
K2O 9.245 %
MgO 1.935 %
Na2O 1.23 %
 
Descriptive Properties
Appearance+75-80, 85, 90Color White
iO20.5687
L.O.I.0.0321

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aclo Accutech Polypropylene Homopolymer HP0334M10L Mica Reinforced
Aclo Accutech Polypropylene Copolymer CP0437M40L Mica Reinforced
Aclo Accutech Polypropylene Copolymer CP0437M10CL Mica Reinforced Coupled
Aclo Accutech Polypropylene Copolymer CP0436M40L Mica Reinforced
Aclo Accutech Polypropylene Copolymer CP0436M10L Mica Reinforced

PCHEMT028 / 194969

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.