MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
VICTREX™ PEEK 450G903 Black Polyetheretherketone, Unreinforced
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Unreinforced

Material Notes: Product Description:

High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, FDA food contact compliant, colour black.

Typical Application Areas:

Applications for high strength and stiffness as well as high ductility. Chemically resistant to aggressive environments, suitable for sterilization for medical and food contact applications.

Information Provided by Victrex.

Vendors: Victrex is a global leader in high-performance PEEK and PAEK polymers, transforming industries from aerospace to medical devices. For 40 years, our innovative polymer solutions help customers achieve new levels of performance, sustainability, and cost efficiency across applications that millions rely on daily from smartphones to aircraft components. As pioneers in polymer engineering, we're committed to delivering transformational solutions that address global materials challenges. Visit www.victrex.com, call (800) VICTREX /1-484-342-6001, or email victrexplc@victrex.com.

Ensinger TECAPEEK™ shapes are manufactured exclusively with Victrex™ PEEK polymer. The Ensinger process and Victrex resins ensure reliability, consistency, dimensional stability, and high temperature mechanical performance.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.30 g/ccCrystalline; ISO 1183
Water Absorption at Saturation 0.40 %
@Temperature 23.0 °C
ISO 62-1
 0.56 %
@Temperature 100 °C
ISO 62-1
Viscosity 350000 cP
@Temperature 400 °C
melt; ISO 11443
Linear Mold Shrinkage, Flow 0.010 cm/cm375°C nozzle, 180°C tool; ISO 294-4
Linear Mold Shrinkage, Transverse 0.013 cm/cm375°C nozzle, 180°C tool; ISO 294-4
Spiral Flow 11.0 cm
@Thickness 1.00 mm
Mold Temp: 180°C, Melt Temp: 375°C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 85
@Temperature 23.0 °C
ISO 868
Tensile Strength, Yield 98.0 MPa
@Temperature 23.0 °C
ISO 527
Elongation at Break 30 %
@Temperature 23.0 °C
ISO 527
Tensile Modulus 3.80 GPa
@Temperature 23.0 °C
ISO 527
Flexural Strength 12.5 MPa
@Temperature 275 °C
ISO 178
 19.0 MPa
@Temperature 175 °C
ISO 178
 85.0 MPa
@Temperature 125 °C
ISO 178
 165 MPa
@Temperature 23.0 °C
ISO 178
 125 MPa
@Strain 3.5 %,
Temperature 23.0 °C
ISO 178
Flexural Modulus 3.80 GPa
@Temperature 23.0 °C
ISO 178
Compressive Strength 70.0 MPa
@Temperature 120 °C
ISO 604
 125 MPa
@Temperature 23.0 °C
ISO 604
Izod Impact, Notched (ISO) 7.00 kJ/m²
@Temperature 23.0 °C
ISO 180/A
Izod Impact, Unnotched (ISO) NB
@Temperature 23.0 °C
ISO 180/U
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+9 ohm-cm
@Temperature 275 °C
IEC 60093
 1.00e+15 ohm-cm
@Temperature 125 °C
IEC 60093
 1.00e+16 ohm-cm
@Temperature 23.0 °C
IEC 60093
Dielectric Constant 2.9
@Frequency 1000 Hz
IEC 60250
Dielectric Strength 24.0 kV/mm
@Thickness 2.00 mm
IEC 60243-1
Dielectric Loss Index 0.0040
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 150 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear 55.0 µm/m-°C
@Temperature <=143 °C
Average below Tg; ISO 11359
 140 µm/m-°C
@Temperature >=143 °C
Average above Tg; ISO 11359
CTE, linear, Parallel to Flow 45.0 µm/m-°C
@Temperature <=143 °C
Below Tg; ISO 11359
 120 µm/m-°C
@Temperature >=143 °C
Above Tg; ISO 11359
CTE, linear, Transverse to Flow 55.0 µm/m-°C
@Temperature <=143 °C
Below Tg; ISO 11359
 140 µm/m-°C
@Temperature >=143 °C
Above Tg; ISO 11359
Thermal Conductivity 0.320 W/m-KAlong flow; ISO 22007-4
 0.290 W/m-K
@Temperature 23.0 °C
Average; ISO/CD 22007-4
Melting Point 343 °CISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 152 °CISO 75-f
Glass Transition Temp, Tg 143 °COnset; ISO 11357
 150 °CMidpoint; ISO 11357
UL RTI, Electrical 260 °CUL 746B
UL RTI, Mechanical with Impact 180 °CUL 746B
UL RTI, Mechanical without Impact 240 °CUL 746B
Glow Wire Flammability Index 960 °C
@Thickness 2.00 mm
IEC 60695-2-12
 
Processing PropertiesOriginal ValueComments
Processing Temperature <= 100 °CHopper Temperature
Rear Barrel Temperature 355 °C
Middle Barrel Temperature 360 - 365 °C
Front Barrel Temperature 370 °C
Nozzle Temperature 375 °C
Mold Temperature 170 - 200 °C
Drying Temperature 120 - 150 °C
@Time 10800 - 18000 sec
 
Descriptive Properties
Gate>1 mm or 0.5 x part thickness
Runner>3.5mmmanifold
 >3mm Die/nozzle

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
VICTREX™ PEEK 450G™ General Purpose
VICTREX™ PEEK 150G / 151G Polyetheretherketone, Unreinforced
VICTREX™ PEEK 381G Medium Viscosity
VICTREX™ PEEK 150P Polyetheretherketone, Unreinforced
VICTREX™ PEEK 450CA30 30% Carbon Fiber Reinforced

PVICTA60 / 99738

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.