MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ExxonMobil Exxtra™ Seal POP 229 Plastomer for Cast Film
Categories: Polymer; Film; Thermoplastic; Elastomer, TPE

Material Notes: Product Description: Exxtra™ Seal POP 2295 is an ethylene-based hexene plastomer produced using ExxonMobil Chemical's EXXPOL® Catalyst Technology. Seal POP2295 is designed for both monolayer and multilayer coextruded cast and blown film applications requiring low sealing temperatures, high oxygen transmission and high toughness. Typical applications include seal layers for lamination films used in meat, poultry and produce packaging

Availability: Latin America, North America

Additive:

  • Antiblock: No
  • Slip: No
  • Thermal Stabilizer: Yes
Applications:
  • Cast Film
  • Lamination Film
Information provided by ExxonMobil Chemical

Key Words: EXACT™ 4151
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.895 g/ccExxonMobil Method
Thickness 1.00 mil
Melt Flow 2.2 g/10 min190°C/2.16kg; ExxonMobil Method
 
Mechanical PropertiesOriginal ValueComments
Puncture Resistance 17.0 lb (f)ExxonMobil Method
Film Tensile Strength at Yield, MD 900 psiASTM D882
Film Tensile Strength at Yield, TD 480 psiASTM D882
Film Elongation at Break, MD 360 %ASTM D882
Film Elongation at Break, TD 650 %ASTM D882
Puncture Energy 55.0 in-lbExxonMobil Method
Elmendorf Tear Strength, MD 110 g/milASTM D1922
Elmendorf Tear Strength, TD 400 g/milASTM D1922
Dart Drop 800 g/milASTM D1709A
Film Tensile Strength at Break, MD 11000 psiASTM D882
Film Tensile Strength at Break, TD 8000 psiASTM D882
1% Secant Modulus, MD 7000 psiASTM D882
1% Secant Modulus, TD 8900 psiASTM D882
 
Thermal PropertiesOriginal ValueComments
Melting Point 190 °FPeak Melting Temperature; ExxonMobil Method
Crystallization Temperature 71.0 °CExxonMobil Method
Vicat Softening Point 169 °FASTM D1525
 
Optical PropertiesOriginal ValueComments
Haze 0.50 %ASTM D1003
Gloss 91 %ASTM D2457
 
Descriptive Properties
Puncture Force13 lbfExxonMobil Method

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DuPont Teijin Films Mylar® 50 OL2 Polyester Film, 50 Gauge
Westlake EC 475 Low Density Polyethylene
NatureWorks® Ingeo™ 4032D Film Grade PLA
Lotte Chemical Titan TITANLENE® LDC801YY Low density polyethylene resin
Eastman 9921W PET Film

PEXB353 / 37658

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.