MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Meldin Supplier

(Viewing data as-entered. Click here to return)
DuPont Mobility and Materials Vespel® SF-0920 Polyimide Foam, Low Density
Categories: Polymer; Thermoplastic; Polyimide, Thermoplastic

Material Notes: Vespel® SF foam products are ideal candidates for applications requiring extremes of strength, temperature, and performance. Vespel® SF foam products are characterized by high compressive strength, excellent insulative properties, and outstanding resistance to heat, fire, solvents, and chemicals. Additional properties include increased stiffness and low weight.

Applications: Potential applications may include:
AERO-ENGINES & AERO-FRAMES:

  • Stator vanes seals
  • Variable bushing packing
  • Nacelle insulation
  • Reinforced composite panels

INDUSTRIAL MARKETS
  • Machinery
  • Vibration isolation for oven shelves
  • Material handling equipment
  • High temperature gaskets

TRANSPORTATION MARKETS
  • General aviation, ultralight composite aircraft
  • Automotive (commercial & racing)

Properties are typical and not legally guaranteed.

Information provided by DuPont

Information provided by DuPont. This product line has remained with DuPont after the DuPont-Dow merger.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 9.06 - 9.66 lb/ft³ASTM D3574 Test E
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 61.6 psiASTM D3574 Test E
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 1.11ASTM D1673
Dissipation Factor 0.00252pf.; ASTM D1673
 
Thermal PropertiesOriginal ValueComments
CTE, linear 0.130 µin/in-°F
@Temperature 54.4 - 93.3 °C
ASTM E228
 0.280 µin/in-°F
@Temperature 15.6 - 54.4 °C
ASTM E228
Thermal Conductivity 0.0330 - 0.0360 W/m-K25°C (77°F); ASTM C518
Maximum Service Temperature, Air 300 °C
 
Descriptive Properties
Compressive Force Test @20%, psi17.4ASTM D3574 Test C
Compressive Force Test @40%, psi29ASTM D3574 Test C
Max Standard Thickness, in.1.42
Standard Sheet Size, in.~23x23

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
3A Composites Core Materials AIREX® C71.75 Elevated Temperature Structural Foam
Armacell ArmaFORM® FR100 PET foam core
DIAB Rigid Foam IPN 20-649 Type 1
DuPont Mobility and Materials Vespel® SF-0940 Polyimide Foam, High Density
Evonik Solimide® HT-340 Polyimide Foam

PDU2011 / 32873

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.