MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Overview of materials for Silver Alloy
Categories: Metal; Nonferrous Metal; Precious Metal; Silver Alloy

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Silver Alloy". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 3.50 - 16.0 g/ccAverage value: 10.4 g/cc Grade Count:298
Viscosity 90000 - 750000 cPAverage value: 304000 cP Grade Count:7
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 82.0 - 161Average value: 108 Grade Count:7
Hardness, Knoop 92.0 - 1010Average value: 319 Grade Count:9
Hardness, Rockwell B 35.0 - 102Average value: 73.9 Grade Count:60
Hardness, Rockwell F 3.00 - 90.0Average value: 58.7 Grade Count:42
Hardness, Rockwell 15T 44.0 - 87.0Average value: 69.9 Grade Count:20
Hardness, Vickers 25.0 - 280Average value: 146 Grade Count:28
Tensile Strength, Ultimate 83.0 - 896 MPaAverage value: 325 MPa Grade Count:142
Tensile Strength, Yield 54.0 - 730 MPaAverage value: 369 MPa Grade Count:29
Elongation at Break 0.000 - 55.0 %Average value: 15.3 % Grade Count:97
Reduction of Area 0.000 - 90.0 %Average value: 39.0 % Grade Count:5
Modulus of Elasticity 10.0 - 105 GPaAverage value: 81.0 GPa Grade Count:29
Compressive Yield Strength 207 - 339 MPaAverage value: 297 MPa Grade Count:5
Poissons Ratio 0.360 - 0.390Average value: 0.370 Grade Count:4
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000147 - 0.000784 ohm-cmAverage value: 0.00000951 ohm-cm Grade Count:239
Surface Resistance 0.00250 - 0.00300 ohmAverage value: 0.00283 ohm Grade Count:3
 
Thermal PropertiesOriginal ValueComments
CTE, linear 15.4 - 22.4 µm/m-°CAverage value: 19.0 µm/m-°C Grade Count:51
Specific Heat Capacity 0.230 - 0.234 J/g-°CAverage value: 0.232 J/g-°C Grade Count:11
Thermal Conductivity 2.00 - 425 W/m-KAverage value: 244 W/m-K Grade Count:61
Melting Point 525 - 3410 °CAverage value: 868 °C Grade Count:350
Solidus 525 - 1150 °CAverage value: 742 °C Grade Count:293
Liquidus 525 - 3410 °CAverage value: 959 °C Grade Count:318
Boiling Point 2160 - 2210 °CAverage value: 2180 °C Grade Count:5
Maximum Service Temperature, Air 149 - 961 °CAverage value: 285 °C Grade Count:26
 
Processing PropertiesOriginal ValueComments
Processing Temperature 600 - 1090 °CAverage value: 800 °C Grade Count:111
Casting Temperature 940 - 1300 °CAverage value: 1140 °C Grade Count:10
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 0.00200 - 5.00 %Average value: 2.75 % Grade Count:4
Cadmium, Cd 0.00100 - 25.0 %Average value: 13.4 % Grade Count:56
Carbon, C 0.00500 - 10.0 %Average value: 1.40 % Grade Count:25
CdO 10.0 - 20.0 %Average value: 13.5 % Grade Count:18
Copper, Cu 0.0500 - 99.9 %Average value: 25.8 % Grade Count:260
Gold, Au 2.00 - 75.0 %Average value: 47.2 % Grade Count:18
Indium, In 0.600 - 15.0 %Average value: 10.3 % Grade Count:16
Iridium, Ir 0.100 - 0.300 %Average value: 0.150 % Grade Count:4
Iron, Fe 0.00500 - 10.0 %Average value: 6.67 % Grade Count:3
Lead, Pb 0.00200 - 60.0 %Average value: 4.00 % Grade Count:15
Lithium, Li 0.150 - 0.500 %Average value: 0.284 % Grade Count:5
Magnesium, Mg 0.200 - 0.250 %Average value: 0.236 % Grade Count:7
Manganese, Mn 1.50 - 16.0 %Average value: 6.77 % Grade Count:20
Molybdenum, Mo 50.0 - 65.0 %Average value: 60.0 % Grade Count:8
Nickel, Ni 0.00200 - 30.0 %Average value: 3.48 % Grade Count:86
Palladium, Pd 1.00 - 50.0 %Average value: 16.4 % Grade Count:45
Phosphorus, P 0.00200 - 1.20 %Average value: 0.0797 % Grade Count:14
Platinum, Pt 0.400 - 12.0 %Average value: 4.10 % Grade Count:9
Silicon, Si 0.200 %Average value: 0.200 % Grade Count:3
Silver, Ag 19.0 - 100 %Average value: 60.6 % Grade Count:418
Tin, Sn 1.50 - 10.5 %Average value: 4.90 % Grade Count:55
Titanium, Ti 1.25 - 10.0 %Average value: 4.39 % Grade Count:11
Tungsten, W 10.0 - 78.0 %Average value: 58.4 % Grade Count:35
WC 42.0 - 60.0 %Average value: 52.1 % Grade Count:10
Zinc, Zn 0.00100 - 37.0 %Average value: 18.7 % Grade Count:163

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Copper Alloy
Overview of materials for Aluminum Alloy
Overview of materials for Nickel Alloy
Overview of materials for Gold Alloy
Overview of materials for Tungsten Alloy

M01066 / 81697

Metalmen Sales

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.