MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Schott NanoFine 180 Dental Glass
Categories: Ceramic; Glass; Oxide; Silicon Oxide

Material Notes: NanoFine 180 falls between UltraFine powders and the common nano powders, this grain size can open up new dimensions of filler load, transparency and polishability.

    Advantages
  • First refractive index matching radiopaque glass < 200 nm (d50)
  • Ideal compatibility to the established GM27884 powders
  • Extremely narrow grain size distribution
  • Easy to disperse

Information Provided by SCHOTT North America, Inc.

Key Words: GM27884
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.80 g/cc
Grain Size 0.15 - 0.21 µmd50
 <= 0.50 µmd99
 
Thermal PropertiesOriginal ValueComments
CTE, linear 4.00 µm/m-°C
@Temperature -30.0 - 70.0 °C
Transformation Temperature, Tg 665 °C
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.53
@Wavelength 587.6 nm
nd
 
Component Elements PropertiesOriginal ValueComments
Al2O3 10 %
B2O3 10 %
BaO 25 %
SiO2 55 %
 
Descriptive Properties
Hydrolytic ResistanceClass 1DIN ISO 719
Radiopacity as thickness of aluminum equal to 2-mm thick glass material4.2ISO 4049

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Schott GM27884 Dental Glass
Vibrantz Technologies IX 2693 Dental Glass
CeramTec ATZ Alumina Toughened Zirconia, Dental Grade
Vibrantz Technologies IX 1944 Dental Glass
Vibrantz Technologies EG 2738 Dental Glass

CSGS111 / 93445

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.