MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LyondellBasell Hostalen CRP 100 ORANGE High Density Polyethylene (HDPE), Pipe Grade
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Pipe Grade

Material Notes: Hostalen CRP 100 orange is a high density polyethylene (HDPE), orange colored similar RAL 1033 with high melt viscosity for extrusion and injection molding. The product is classified as PE 100 and provides excellent stress crack resistance properties (ESCR) combined with very good long term hydrostatic strength. The compound fulfills the material requirements of EN 1555-1 and ISO 4437-1. Applications: Gas Pipe

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.951 g/ccISO 1183-1
Oxidative Induction Time (OIT) 30 min
@Temperature 210 °C
ISO 11357-6
Melt Flow 0.23 g/10 min
@Load 5.00 kg,
Temperature 190 °C
ISO 1133-1
 6.4 g/10 min
@Load 21.6 kg,
Temperature 190 °C
ISO 1133-1
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 62
@Time 3.00 sec
ISO 868
Tensile Strength, Yield 23.0 MPa50mm/min; ISO 527-1,-2
Elongation at Break >= 350 %ISO 527-1,-2
Elongation at Yield 9.0 %50mm/min; ISO 527-1,-2
Tensile Modulus 1050 MPaISO 527-1,-2
Charpy Impact, Notched 15.0 kJ/m²
@Temperature -30.0 °C
ISO 179-1/1eA
 29.0 kJ/m²
@Temperature 23.0 °C
ISO 179-1/1eA
Tensile Creep Modulus, 1000 hours 360 MPa
@Pressure 2.00 MPa
ISO 899-1
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 74.0 °CB50; ISO 306
DSC Induction Temperature 129 °CDSC
 
Descriptive Properties
FNCT (hrs)>1000ISO 16770, 4.0 MPa, 2% Arkopal N100, 80°C
MRS Classification (MPA)10ISO 9080
Processing Methodpipe

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LyondellBasell Hostalen CRP 100 RESIST S BROWN High Density Polyethylene (HDPE), Pipe Grade
LyondellBasell Hostalen CRP 100 RESIST S BLUE High Density Polyethylene (HDPE), Pipe Grade
LyondellBasell Hostalen CRP 100 RESIST CR W BLUE High Density Polyethylene (HDPE), Pipe Grade
LyondellBasell Hostalen CRP 100 RESIST CR orange High Density Polyethylene (HDPE), Pipe Grade
LyondellBasell Petrothene® LM600731X01 High Density Polyethylene, Sheet Extrusion Grade

PEQT8462 / 220097

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.