MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.04 - 1.16 g/cc0.0376 - 0.0419 lb/in³Average value: 1.09 g/cc Grade Count:58
Water Absorption 0.300 - 1.00 %0.300 - 1.00 %Average value: 0.512 % Grade Count:4
Water Absorption at Saturation 0.700 %0.700 %Average value: 0.700 % Grade Count:3
Viscosity 350000 - 600000 cP
@Temperature 220 - 220 °C
350000 - 600000 cP
@Temperature 428 - 428 °F
Average value: 475000 cP Grade Count:2
Linear Mold Shrinkage 0.00300 - 0.00800 cm/cm0.00300 - 0.00800 in/inAverage value: 0.00537 cm/cm Grade Count:40
Melt Flow 0.300 - 45.0 g/10 min0.300 - 45.0 g/10 minAverage value: 17.6 g/10 min Grade Count:59
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 37.0 - 54.037.0 - 54.0Average value: 45.7 Grade Count:3
Hardness, Rockwell R 78.0 - 11678.0 - 116Average value: 107 Grade Count:35
Ball Indentation Hardness 70.0 - 95.0 MPa10200 - 13800 psiAverage value: 77.4 MPa Grade Count:8
Tensile Strength, Ultimate 30.0 - 57.0 MPa4350 - 8270 psiAverage value: 43.8 MPa Grade Count:25
Tensile Strength, Yield 30.4 - 55.9 MPa4410 - 8110 psiAverage value: 44.3 MPa Grade Count:41
Elongation at Break 10.0 - 70.0 %10.0 - 70.0 %Average value: 28.7 % Grade Count:43
Elongation at Yield 3.50 - 6.00 %3.50 - 6.00 %Average value: 4.38 % Grade Count:13
Modulus of Elasticity 1.35 - 2.35 GPa196 - 341 ksiAverage value: 1.91 GPa Grade Count:12
Flexural Yield Strength 47.1 - 92.2 MPa6830 - 13400 psiAverage value: 67.3 MPa Grade Count:54
Flexural Modulus 1.37 - 2.76 GPa199 - 400 ksiAverage value: 2.09 GPa Grade Count:53
Izod Impact, Notched 0.0981 - 3.04 J/cm0.184 - 5.70 ft-lb/inAverage value: 1.28 J/cm Grade Count:42
 0.200056 - 1.30 J/cm
@Temperature -30.0 - 0.000 °C
0.374786 - 2.44 ft-lb/in
@Temperature -22.0 - 32.0 °F
Average value: 0.640 J/cm Grade Count:5
 0.200056 - 1.30 J/cm
@Thickness 3.17 - 6.40 mm
0.374786 - 2.44 ft-lb/in
@Thickness 0.125 - 0.252 in
Average value: 0.640 J/cm Grade Count:5
Izod Impact, Unnotched  0.392266 - 0.392266 J/cm
@Temperature -30.0 - -30.0 °C
0.734875 - 0.734875 ft-lb/in
@Temperature -22.0 - -22.0 °F
Average value: 0.392 J/cm Grade Count:1
 0.392266 - 0.392266 J/cm
@Thickness 3.20 - 6.40 mm
0.734875 - 0.734875 ft-lb/in
@Thickness 0.126 - 0.252 in
Average value: 0.392 J/cm Grade Count:1
Izod Impact, Notched (ISO) 10.0 - 14.9 kJ/m²4.76 - 7.09 ft-lb/in²Average value: 12.6 kJ/m² Grade Count:5
 7.98 - 7.98 kJ/m²
@Temperature -30.0 - -30.0 °C
3.80 - 3.80 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 7.98 kJ/m² Grade Count:1
Charpy Impact Unnotched 5.10 - 18.0 J/cm²24.3 - 85.7 ft-lb/in²Average value: 11.9 J/cm² Grade Count:7
 6.00 - 12.0 J/cm²
@Temperature -40.0 - -30.0 °C
28.6 - 57.1 ft-lb/in²
@Temperature -40.0 - -22.0 °F
Average value: 8.00 J/cm² Grade Count:6
Charpy Impact, Notched 0.500 - 10.7 J/cm²2.38 - 50.9 ft-lb/in²Average value: 1.43 J/cm² Grade Count:21
 0.200 - 0.798 J/cm²
@Temperature -40.0 - -20.0 °C
0.952 - 3.80 ft-lb/in²
@Temperature -40.0 - -4.00 °F
Average value: 0.337 J/cm² Grade Count:8
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+11 - 1.00e+16 ohm-cm1.00e+11 - 1.00e+16 ohm-cmAverage value: 4.57e+15 ohm-cm Grade Count:7
Surface Resistance 1.00e+11 - 1.00e+15 ohm1.00e+11 - 1.00e+15 ohmAverage value: 5.07e+14 ohm Grade Count:10
Dielectric Constant 2.80 - 3.002.80 - 3.00Average value: 2.92 Grade Count:5
Dissipation Factor 0.0130 - 0.01600.0130 - 0.0160Average value: 0.0148 Grade Count:5
 
Thermal PropertiesMetricEnglishComments
CTE, linear 80.0 - 121 µm/m-°C44.4 - 67.2 µin/in-°FAverage value: 102 µm/m-°C Grade Count:9
Thermal Conductivity 0.170 W/m-K1.18 BTU-in/hr-ft²-°FAverage value: 0.170 W/m-K Grade Count:4
Maximum Service Temperature, Air 75.0 - 90.0 °C167 - 194 °FAverage value: 86.0 °C Grade Count:5
Deflection Temperature at 0.46 MPa (66 psi) 80.0 - 94.0 °C176 - 201 °FAverage value: 90.6 °C Grade Count:9
Deflection Temperature at 1.8 MPa (264 psi) 65.0 - 96.0 °C149 - 205 °FAverage value: 81.0 °C Grade Count:48
Vicat Softening Point 80.0 - 106 °C176 - 223 °FAverage value: 93.0 °C Grade Count:29
UL RTI, Electrical 50.0 - 60.0 °C122 - 140 °FAverage value: 52.7 °C Grade Count:7
UL RTI, Mechanical with Impact 50.0 - 60.0 °C122 - 140 °FAverage value: 52.7 °C Grade Count:7
UL RTI, Mechanical without Impact 50.0 - 60.0 °C122 - 140 °FAverage value: 52.7 °C Grade Count:7
Flammability, UL94 HB - V-2HB - V-2Grade Count:44
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.52 - 1.541.52 - 1.54Average value: 1.54 Grade Count:6
Haze 1.20 - 95.5 %1.20 - 95.5 %Average value: 13.4 % Grade Count:35
Transmission, Visible 6.50 - 90.0 %6.50 - 90.0 %Average value: 81.3 % Grade Count:43
UV Transmittance 91.0 %91.0 %Average value: 91.0 % Grade Count:3
 
Processing PropertiesMetricEnglishComments
Processing Temperature 190 - 265 °C374 - 509 °FAverage value: 222 °C Grade Count:8
Nozzle Temperature 200 - 260 °C392 - 500 °FAverage value: 224 °C Grade Count:13
Adapter Temperature 235 - 245 °C455 - 473 °FAverage value: 240 °C Grade Count:4
Die Temperature 113 - 118 °C235 - 245 °FAverage value: 116 °C Grade Count:4
Melt Temperature 180 - 260 °C356 - 500 °FAverage value: 221 °C Grade Count:20
Mold Temperature 40.0 - 80.0 °C104 - 176 °FAverage value: 56.6 °C Grade Count:24
Injection Velocity 200 mm/sec7.87 in/secAverage value: 200 mm/sec Grade Count:4
Roll Temperature 75.0 - 95.0 °C167 - 203 °FAverage value: 85.0 °C Grade Count:4
Drying Temperature 70.0 - 90.0 °C158 - 194 °FAverage value: 77.3 °C Grade Count:19
Moisture Content 0.0100 - 0.100 %0.0100 - 0.100 %Average value: 0.0325 % Grade Count:4
Injection Pressure 4.83 - 150 MPa700 - 21800 psiAverage value: 73.3 MPa Grade Count:10

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Extruded
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded
Overview of materials for Cellulose Acetate, Molded

O1105 / 77796

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.