MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
CHT Group QGel 310 QSI Quantum Silicones High Strength Gel
Categories: Fluid; Polymer; Thermoset; Silicone

Material Notes: QGel 310 is a clear, very soft, tough moderately cross-linked silicone polymer. Silicone gels are used to provide protection from vibration and thermal or mechanical shock. Silicone gels also provide excellent moisture protection.

Key Features:

  • 24 hour room temperature or heat cure
  • One to one mix ratio
  • Soft but resilient
  • Dispensing equipment not necessary
Part of the Amber Chemical Group. Data provided by manufacturer.

Formerly Amber Chemical Co (ACC Silicones), aquired by CHT in 2017

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.970 g/cc"B" component
 0.970 g/cc"A" component
Viscosity 1000 cP"B" component
 1000 cP"A" component
Storage Temperature <= 38.0 °C12 months
 
Mechanical PropertiesOriginal ValueComments
Penetration 5.0 - 9.0mm, 30 mins @ 150°C
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 487 V/mil
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 200 °C
Minimum Service Temperature, Air -55.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 0.500 hour
@Temperature 150 °C
 1.00 hour
@Temperature 100 °C
 24.0 hour
@Temperature 25.0 °C
Gel Time 45.0 min
 
Descriptive Properties
ColorTransparent"A" component
 Transparent"B" component

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Oxygen-free electronic Copper, UNS C10100
Multibase TPSiV® 3010-60A Thermoplastic Silicone Vulcanizate
Silikony Polskie Polsil Gum 100/40 HTV Silicone Rubber
Silikony Polskie Gumosil B Silicone Rubber
Elkem (Bluestar Silicones) BLUESIL™ GUM 795 Silicone Gum

PACC044 / 22171

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.