MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
DuPont Styrofoam™ Tongue and Groove Extruded Polystyrene Foam Insulation
Categories: Polymer; Thermoplastic; Polystyrene (PS); Expanded Polystyrene (EPS)

Material Notes: STYROFOAM™ Brand Tongue and Groove Insulation features tongue and groove edges on all four sides of 2’ x 8’ boards 1” thick or less and on the long edges of all other boards. The lightweight, moisture-resistant and thermally efficient Type IV extruded polystyrene foam insulation is suited for a wide range of residential and commercial construction applications. STYROFOAM™ Brand Tongue and Groove Extruded Polystyrene Foam Insulation (XPS) goes up quickly and easily with groves on all four edges to lock into the next sheet and gives more coverage per board. It’s easy to install with high compressive strength for above and below grade applications including:
  • Exterior walls
  • Interior walls
  • Ceiling
  • Exterior foundation walls
  • Interior foundation walls
  • Crawl space
STYROFOAM™ Brand Tongue and Groove Insulation is suitable for use in pervious, semi-pervious and practically impervious soils.

This material is produced as sheets of closed-cell foam by a continuous extrusion process. Its properties will be different than expanded polystyrene beads because beads have voids between cell walls.

This former Dow product line is now a DuPont product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Water Absorption <= 0.30 %volume%; ASTM C272
 
Mechanical PropertiesOriginal ValueComments
Flexural Strength >= 50.0 psiASTM C203
Compressive Strength >= 25.0 psiASTM D1621
 
Thermal PropertiesOriginal ValueComments
CTE, linear 63.0 µm/m-°C
@Temperature -30.0 - 30.0 °C
ASTM D696
Insulation R Value >= 5.0
@Thickness 25.4 mm,
Temperature 23.9 °C
ASTM C518
 >= 5.4
@Thickness 25.4 mm,
Temperature 4.44 °C
ASTM C518
 >= 5.6
@Thickness 25.4 mm,
Temperature -3.89 °C
ASTM C518
Maximum Service Temperature, Air 74.0 °C
 
Descriptive Properties
Water Vapor Permeance1.5 perm MaxASTM E96

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DuPont Styrofoam™ SM Extruded Polystyrene Foam Insulation
DuPont Styrofoam™ Scoreboard Extruded Polystyrene Foam Insulation
DuPont Styrofoam™ Ultra SL Extruded Polystyrene Foam Insulation
DuPont Styrofoam™ Square Edge Extruded Polystyrene Foam Insulation
DuPont Styrofoam™ Polystyrene Rigid Foam Insulation

PDWZ00j / 209618

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.