MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Daikin NEOFLON® AP-231SH PFA
Categories: Polymer; Thermoplastic; Fluoropolymer; Perfluoroalkoxy (PFA); Polyperfluoroalkoxyethylene, Molded/Extruded

Material Notes: Neoflon® PFA AP-231SH is a high purity grade resin especially designed for the semiconductor industry with long-term flexibility and good stress crack resistance. It is suitable for extrusion, compression molding and transfer molding.

Typical Applications: Tubing and linings

Information provided by Daikin.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.12 - 2.17 g/ccASTM D-3307
Bulk Density >= 1.20 g/cc
Melt Flow 1.5 - 2.5 g/10 minASTM D-3307
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break >= 30.0 MPaASTM D-3307
Elongation at Break >= 300 %ASTM D-3307
Compressive Yield Strength 5.00 - 6.00 MPa1% Deformation; ASTM D695
Flex Crack Resistance 2.70e+6Cycles per MIT Flex; ASTM D2176
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity <= 1.00e+18 ohm-cmASTM D257
Dielectric Constant 2.1
@Frequency 1000 Hz
ASTM D150
 2.1
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 500 - 600 V/mil
@Thickness 3.17 mm
Short Time; ASTM D149
Dissipation Factor 0.000010
@Frequency 1000 Hz
ASTM D150
 0.00030
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
Melting Point 300 - 310 °CASTM D-3307
Maximum Service Temperature, Air 260 °CContinuous
Minimum Service Temperature, Air -200 °C
Oxygen Index >= 95 %ASTM D2863

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Daikin NEOFLON® AP-201 PFA
Daikin NEOFLON® AP-230 PFA
Daikin NEOFLON® AP-201SH PFA
Daikin NEOFLON® AP-210 PFA
Daikin NEOFLON® AP-211SH PFA

PDAIJ9922 / 209993

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.