MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Buckeye Polymers BP RPP 4010 T NAT Polypropylene, Talc Filled
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 40% Talc Filler

Material Notes: Product Information: Our Talc filled product lines exhibit excellent properties such as high stiffness, surface aesthetics, low coefficient of thermal expansion, low shrinkage, improved scratch and mar resistance, and resistance to some aggressive chemical agents. Buckeye Polymers can also customize these materials through the addition of UV packages, custom color matching, and processing additives.

    Product Features:
  • Increased stiffness and heat deflection
  • Industrial, appliance, construction markets
  • Good scratch and mar resistance
  • Appearance: Translucent

    Forms: Pellets

    Processing Method: Injection Molding

    Information Provided by Buckeye Polymers, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.22 - 1.28 g/ccASTM D792
Melt Flow 10 - 16 g/10 minASTM D1238
Ash 38 - 43 %ASTM D5630
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield >= 4500 psiASTM D638
Flexural Modulus >= 575000 psiASTM D790
Izod Impact, Notched >= 0.600 ft-lb/inASTM D256

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
A. Schulman POLYFLAMâ„¢ FPP 1007 Talc Filled Homopolymer Polypropylene
Aclo Accutech Polypropylene Homopolymer HP0334T40L1 Talc Reinforced
Buckeye Polymers BP RPP 4010 TU NAT Polypropylene, Talc Filled
RTP Company RTP 127 HB Polypropylene (PP), Talc - UL94 HB
A. Schulman Diamond NPP30-2000 GF30 30% Glass Filled Homopolymer Polypropylene

PBUCK036 / 104503

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.