MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
Tra-Con Tra-Bond 2119 Low Viscosity Glass Laminating Adhesive
Categories: Polymer; Adhesive; Thermoset

Material Notes: TRA-BOND 2119 is a crystal clear adhesive specifically designed for bonding glass to glass and glass to plastics. It also yields a high lap shear strength to metals and ceramics. This system cures to a semi-rigid hardness making it ideal for bonding dissimilar substrates especially when thermal cycling is required. This two part adhesive also has a low exotherm and therefore can be used for small pottings and filling bond gaps up to 1/8 inch.

Information provided by Tra-Con Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.06 g/ccMixed
Volatile Organic Compounds (VOC) Content 87.7 g/l
Water Absorption 0.49 %After 24 hours
Viscosity 500 cP
@Temperature 25.0 °C
Mixed (sp #4, 12 rpm)
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 7624 hrs @ 25°C
 791 hr @ 65°C
 802 hrs @ 65°C
Adhesive Bond Strength 1750 psiLap shear, alum to alum, 24 hrs @ 25°C
 2300 psiLap shear, alum to alum, 1 hr @ 65°C
 2650 psiLap shear, alum to alum, 2 hrs @ 65°C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 88.8 µm/m-°CBelow Tg
 241 µm/m-°CAbove Tg
Glass Transition Temp, Tg 95.0 °CUltimate Tg
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.53
 
Processing PropertiesOriginal ValueComments
Cure Time 1.00 - 2.00 hour
@Temperature 65.0 °C
 24.0 hour
@Temperature 25.0 °C
Pot Life 45 min25 grams
Working Life 2.00 hour25 grams
 
Descriptive Properties
Color Clear
Thixotropic Index 16 rpm/60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Master Bond EP45HTQ Quartz Filled Heat Resistant Epoxy
Master Bond EP30QF Quartz filled, Two Part Epoxy System
Dymax 4-425 Glass Bonding Adhesive
Dow 733 GLASS & METAL SEALANT
Rogers Arlon Secure™ 48A50B020 0.020" Thermally Conductive Silicone Rubber Adhesive on Fiberglass for Solar Cell Encapsulation

PTRAC018 / 70946

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.